MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Coosa Composites Bluewater 26 20 mm Fiberglass Reinforced Polyurethane Foam Panel
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Glass Filled

Material Notes: The Bluewater composite panels are made from high-density closed-cell polyurethane foam reinforced with continuous strand fiberglass and woven roving. They’re used for lightweight building applications that previously called for the use of plywood. The Bluewater series is ideal for projects in marine or high-humidity settings. It is also suitable for applications that require a high strength per cubic foot ratio with the added benefit of being lighter than plywood.

Bluewater 26: Boasting an impressive strength-to-weight ratio, the Bluewater 26 stands out as one of Coosa's most durable panels. The combination of woven roving and continuous fiberglass strands ensures remarkable stiffness. Notably, the Bluewater 26 is not only strong but also weighing over 30% less than plywood alternatives. Their minimal water absorption makes them an ideal choice for applications requiring a product that is rot-resistant, lightweight, and exceptionally durable.

Information provided by Coosa Composites

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.417 g/cc0.0150 lb/in³ASTM C271
Water Absorption 1.10 %1.10 %ASTM C272
Thickness 20000 microns787 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 3.30 MPa479 psiFlatwise; ASTM C297
Flexural Strength 34.2 MPa4960 psiASTM D790
Flexural Modulus 1.675 GPa242.9 ksiASTM D790
Compressive Strength 5.70 MPa827 psiCore; ASTM C365
Compressive Modulus 0.0814 GPa11.8 ksiCore; ASTM C365
Shear Modulus 0.0291 GPa4.22 ksiCore; ASTM C273
Shear Strength 3.70 MPa537 psiCore; ASTM C273

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOOS901 / 322921

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.