MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

DuPont™ Clysar® VHP Polyolefin Shrink Packaging Film, 50 Gauge  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyolefin; Polyolefin, Film Grade; Polyolefin, Film Grade (Polyolefin)

Material Notes: Data provided by DuPont Packaging Polymers.

DuPont Clysar® VHP is a thin gauge, clear, biaxially oriented, heat shrinkable polyolefin film. It provides strong seals and excellent optics under a wide range of operating conditions.

DuPont Clysar® VHP is designed for the packaging of lightweight, low-abuse products. It combines excellent optics and seal strength with the economics of high yield, reduced changeover and downtime, and greater use of storage space.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Moisture Vapor Transmission 0.440 cc-mm/m²-24hr-atm1.12 cc-mil/100 in²-24hr-atmASTM 1249
Oxygen Transmission 236 cc-mm/m²-24hr-atm599 cc-mil/100 in²-24hr-atmor 14100 cc/m²-24hr-atm for the 50 gauge film. ASTM D3985
Thickness 12.7 microns0.500 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 115 %115 %Average; ASTM D882
Secant Modulus 0.410 GPa59.5 ksiStiffness Modulus; ASTM D882
Impact Test 1.13 J0.833 ft-lbSpencer Impact ASTM D3420
Coefficient of Friction, Dynamic 0.300.30ASTM D1894
Elmendorf Tear Strength MD 15 g15 gOrientation not specified; ASTM D1922
Film Tensile Strength at Break, MD 103 MPa14900 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 15 %15 %ASTM D1003
Gloss 145 %145 %at 20°; ASTM D2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDU7A2 / 33192

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.