MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Braskem LF118 LLDPE Blown Film Extrusion Polyethylene Copolymer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Butene, Film

Material Notes: LF118 is a linear low-density polyethylene, copolymer of butene-1, produced by the gas phase process. It is developed for blown film extrusion in blends with polyethylene. Films obtained with this product show a good processing performance balanced with good mechanical properties as well as sealability. It contains antioxidant additives. Its applications include: stretch films, liners, and LDPE and HDPE blends and packages for general use. Recommended processing conditions for film extrusion are about 170 - 210 ºC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.919 g/cc0.0332 lb/in³ASTM-D1505
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 1120 %1120 %ASTM-D882
Film Elongation at Break, TD 1440 %1440 %ASTM-D882
Elmendorf Tear Strength MD 110 g110 gASTM-D1922
Elmendorf Tear Strength TD 400 g400 gASTM-D1922
Elmendorf Tear Strength, MD 2.89 g/micron73.4 g/milASTM-D1922
Elmendorf Tear Strength, TD 10.53 g/micron267.5 g/milASTM-D1922
Dart Drop 2.89 g/micron73.4 g/milASTM-D1709
Dart Drop Test 110 g0.243 lbASTM-D1709
Film Tensile Strength at Break, MD 50.0 MPa7250 psiASTM-D882
Film Tensile Strength at Break, TD 40.0 MPa5800 psiASTM-D882
1% Secant Modulus, MD 200 MPa29000 psiASTM-D882
1% Secant Modulus, TD 230 MPa33400 psiASTM-D882
 
Optical PropertiesMetricEnglishComments
Haze 9.0 %9.0 %ASTM-D1003
Gloss 120 %120 %Angle 60°; ASTM-D2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBRAS848 / 106694

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.