MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 75 Gauge  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Polyolefin; Polyolefin, Film Grade; Polyolefin, Film Grade (Polyolefin); Polypropylene (PP)

Material Notes: Data provided by DuPont Packaging Polymers.

A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when excellent optics, high shrink force, and superb sheet flatness are essential. An excellent choice for doing multi-packs, high-speed applications, and static sealing.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Oxygen Transmission 97.0 cc-mm/m²-24hr-atm246 cc-mil/100 in²-24hr-atmor 5100 cc/m²-24hr-atm for the film. ASTM D3985
Thickness 19.0 microns0.750 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 130 %130 %Average; ASTM D882
Modulus of Elasticity 0.770 GPa112 ksi(stiffness), ASTM D882
Coefficient of Friction, Dynamic 0.400.40ASTM D1894
Elmendorf Tear Strength MD 6.0 g6.0 gOrientation not specified; ASTM D1922
Seal Strength 2800 g/25 mm2800 g/inF-88-68(73)
Film Tensile Strength at Break, MD 131 MPa19000 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 1.2 %1.2 %
Gloss 130 %130 %
 
Processing PropertiesMetricEnglishComments
Processing Temperature 177 - 232 °C351 - 450 °FOptimum Tunnel temperature range.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kuraray SEPTON® 2043 Thermoplastic Rubber
Covestro Texin® 970 U Thermoplastic Polyurethanes (TPU)
Overview of materials for Chlorosulfonated Polyethylene Rubber
NOVA Chemicals Sclair® 11M1 Butene LLDPE Film Resin
Kuraray SEPTON® S2002 Thermoplastic Rubber

PDU756 / 33172

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.