MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Reynolds Soma Foama® 15 Flexible Platinum Silicone Foams
Categories: Polymer; Thermoset; Silicone; Silicone Foam

Material Notes: Product Overview: Soma Foama® is a soft, two-component platinum silicone flexible foam that is versatile and easy to use. Soma Foama® 15 expands 4 times its original volume and develops a uniform 15 lb./cu. ft. cell structure (240 kg/m³). Soma Foama® 25 is a higher density foam vs. original Soma Foama® 15 which expands 2-3 times its original volume and develops a uniform 25 lb./cu. ft. cell structure (400 kg/m³). Vibrant colors can be achieved by adding Silc-Pig® silicone color pigments. Cured foam is high heat resistance (will resist up to 350°F/176°C), water resistant, UV resistant and resists oxidation and ozone degradation. Soma Foama® can be used for a variety of industrial and special effects applications including making foam filled appliances, padding/seat cushioning, orthotics/orthopedics, potting and encapsulation of electrical circuits and vibration dampening.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.240 g/cc0.240 g/ccASTM D-1475
Viscosity 10000 cP10000 cPMixed; ASTM D-2393
 
Processing PropertiesMetricEnglishComments
Cure Time 20.0 min0.333 hourHandling/Tack-Free Time
 60.0 min1.00 hour
Pot Life 0.500 min0.500 minASTM D-2471
 
Descriptive Properties
Approx. Volumetric Expansion4times
ColorWhite
Kgs./Cubic Meter240[kg/m³]
Lbs./Cubic Foot15[lb/ft³]
Mix Ratio100A:47Bby weight
 2A:1Bby volume
Specific Volume115[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN184 / 296885

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.