MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Syensqo (Solvay Specialty Polymers) Ryton® R-7-121BL Polyphenylene Sulfide (PPS), Glass\Mineral  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

Material Notes: Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional molding equipment.

Good Flow; Good Strength

Uses: Automotive Applications

Processing: Injection Molding

Availability: Asia Pacific; Europe; Latin America; North America

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.95 g/cc1.95 g/ccASTM D792
Water Absorption 0.020 %
@Time 86400 sec
0.020 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm
@Thickness 3.20 mm
0.0020 in/in
@Thickness 0.126 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0040 cm/cm
@Thickness 3.20 mm
0.0040 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 101101ASTM D785
Hardness, Rockwell R 118118ASTM D785
Tensile Strength 117 MPa17000 psiASTM D638
 125 MPa18100 psiISO 527-2
Elongation at Break 0.90 %0.90 %ASTM D638
 0.90 %0.90 %ISO 527-2
Flexural Strength 195 MPa28300 psiISO 178
 200 MPa29000 psiASTM D790
Flexural Modulus 17.2 GPa2490 ksiASTM D790
 18.0 GPa2610 ksiISO 178
Compressive Strength 285 MPa41300 psiASTM D695
Poissons Ratio 0.360.36ASTM E132
Izod Impact, Notched 0.530 J/cm
@Thickness 3.18 mm
0.993 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 2.10 J/cm
@Thickness 3.18 mm
3.93 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²Notch A; ISO 180
Izod Impact, Unnotched (ISO) 14.0 kJ/m²6.66 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Surface Resistance 1.00e+16 ohm1.00e+16 ohmASTM D257
Insulation Resistance 1.00e+11 ohm
@Temperature 90.0 °C
1.00e+11 ohm
@Temperature 194 °F
IEC 60167
Dielectric Constant  4.8
@Frequency 1000 Hz
4.8
@Frequency 1000 Hz
ASTM D150
 4.9
@Frequency 1e+6 Hz
4.9
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 18.0 kV/mm457 kV/inASTM D149
Dissipation Factor  0.0020
@Frequency 1e+6 Hz
0.0020
@Frequency 1e+6 Hz
ASTM D150
 0.0040
@Frequency 1000 Hz
0.0040
@Frequency 1000 Hz
ASTM D150
Arc Resistance 185 sec185 secASTM D495
Comparative Tracking Index 250 V250 VUL 746
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  15.0 µm/m-°C
@Temperature 100 - 200 °C
8.33 µin/in-°F
@Temperature 212 - 392 °F
ASTM E831
 15.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
8.33 µin/in-°F
@Temperature -58.0 - 122 °F
ASTM E831
CTE, linear, Transverse to Flow  30.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
16.7 µin/in-°F
@Temperature -58.0 - 122 °F
ASTM E831
 70.0 µm/m-°C
@Temperature 100 - 200 °C
38.9 µin/in-°F
@Temperature 212 - 392 °F
ASTM E831
Thermal Conductivity 0.580 W/m-K4.03 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 220 - 240 °C428 - 464 °FUL Temperature Rating
Deflection Temperature at 1.8 MPa (264 psi) 265 °C509 °FUnannealed; ASTM D648
Oxygen Index 61 %61 %ASTM D2863
 
Descriptive Properties
ColorBlack
FormsPellets
RoHS ComplianceRoHS Compliant

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LATI Larton G/40 PPS, 40% Glass Fiber Reinforced
LATI Larton CE/60 PPS, 60% Mineral Reinforced
LATI Larton GK/400 PPS, Glass/Carbon Fiber Reinforced

PSOL8Y6383 / 193304

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.