MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

3M Scotchkote™ PR 504 Urethane Pipe Repair
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Liquid

Material Notes: Scotchkote Urethane Pipe Repair PR 504 is a special fast curing moisture activated repair bandage for repair bandage for repairs to leaking pipes.

Product Features:

    Easy to apply, requiring no special tools or equipment. Specially selected woven polyester fabric impregnated with a polyurethane resin which is activated by immersion in water.
  • Ideal for repairing pipes operating at low pressures
  • Designed for use for repairs to pipes up to 65 mm diameter
  • Can be used on a wide variety of surfaces, including all metals and many types of plastic

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 32.0 MPa4640 psi
Compressive Strength 19.00 MPa2755 psi
 
Processing PropertiesMetricEnglishComments
Cure Time 5.0000 min0.083333 hourInitial Set
 30.0 min0.500 hourFull Mechanical
 
Descriptive Properties
AppearanceOff white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35311 / 170058

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.