MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Röhm ACRYLITE® Resist 45 Acrylic Sheet
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Optical Sheet

Material Notes: Continuously manufactured ACRYLITE® Resist sheet is a versatile, thermoplastic material developed for the retail display and glazing markets as well as other markets requiring strength, appearance and weatherability. High optical quality ACRYLITE® Resist sheet provides the beautiful look of acrylic with much greater impact strength for durability during manufacturing, shipping, and in-store use. Rigid, tough, and lightweight, ACRYLITE® Resist is easily fabricated and machined, including cutting, routing, forming, and cementing. ACRYLITE® Resist is ideal for use in:
  • P-O-P Displays
  • Store Fixtures
  • Glazing
  • General Fabrication

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ASTM D729
Water Absorption 0.30 %
@Temperature 23.0 °C,
Time 86400 sec
0.30 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8888ASTM D785
Tensile Strength, Yield 59.2 MPa8590 psiASTM D638
Elongation at Yield 5.8 %5.8 %ASTM D638
Tensile Modulus 2.75 GPa399 ksiASTM D638
Flexural Strength 101.3 MPa14690 psiASTM D790
Flexural Modulus 2.54 GPa368 ksi
Izod Impact, Notched (ISO) 0.660 kJ/m²0.314 ft-lb/in²ASTM D256
Gardner Impact 2.26 J1.67 ft-lbASTM D3029
 
Thermal PropertiesMetricEnglishComments
CTE, linear 126 µm/m-°C70.0 µin/in-°FASTM D969
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C208 °FASTM D648
Vicat Softening Point 103 °C217 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.491.49ASTM D542
Gloss 125 %125 %20°; ASTM D523
Transmission, Visible 91.6 %91.6 %ASTM D1003
 
Descriptive Properties
Charpy Impact740 J/mASTM D5942-97

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röhm Acrylite® 8N Acrylic Polymer
Röhm ACRYLITE® Resist 65 Acrylic Sheet
Plaskolite Duraplex® 50% I Impact Modified Acrylic Sheet
Röhm Acrylite Plus® zdf Impact Acrylic Polymer
Röhm Acrylite Plus® zk3HR Impact Acrylic Polymer

PEVONIL051 / 196255

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.