System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Epoxyset Epoxiohm EO-97M Electrically Conductive Epoxy Adhesive
Categories:
Polymer
;
Adhesive
;
Thermoset
;
Epoxy
;
Epoxy, Electrically Conductive
Material Notes:
EPOXIOHM-97M is one part, pure silver filled, high electrical conductivity, epoxy adhesive. It is designed for microelectronics chip bonding application.
Information provided by Epoxyset Inc.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
3.20
g/cc
0.116
lb/in³
Viscosity
10000
-
15000
cP
10000
-
15000
cP
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
88
88
ASTM D2240
Shear Strength
23.0
MPa
3340
psi
Adhesive Bond Strength
8.96
MPa
1300
psi
Lap Shear Strength
Electrical Properties
Metric
English
Comments
Electrical Resistivity
<=
0.000400
ohm-cm
<=
0.000400
ohm-cm
Thermal Properties
Metric
English
Comments
CTE, linear
56.0
µm/m-°C
31.1
µin/in-°F
Thermal Conductivity
2.00
W/m-K
13.9
BTU-in/hr-ft²-°F
Maximum Service Temperature, Air
200
°C
392
°F
Minimum Service Temperature, Air
-55.0
°C
-67.0
°F
Glass Transition Temp, Tg
89.0
°C
192
°F
Processing Properties
Metric
English
Comments
Cure Time
10.0
min
@Temperature 175 °C
0.167
hour
@Temperature 347 °F
120
min
@Temperature 125 °C
2.00
hour
@Temperature 257 °F
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PEPOXY818 / 150843
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.