MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Von Roll Durapol® F200 SMC Polyester - Glass Laminate
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer, Glass Filled

Material Notes: Highlights: Mechanical properties, 94V-0 halogen-free EN 45545 approved.

Glass mat laminates are manufactured using low-pressure techniques and are characterized using mainly glass mat or chopped glass as a reinforcement material. Delmat® and Durapol® laminates are widely used in the electro-mechanical industries. Von Roll has also developed special qualities for the electronics industry and for thermal protection applications. The products are attractive both for their good mechanical and electrical properties, and their resistance against corrosion at high-temperature levels.

Information provided by Von Roll.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.70 - 1.90 g/cc0.0614 - 0.0686 lb/in³ISO 1183
Water Absorption 0.10 %0.10 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 70.0 MPa10200 psiISO 527
Flexural Strength  70.0 MPa
@Temperature 130 °C
10200 psi
@Temperature 266 °F
flatwise; ISO 178
 130 MPa
@Temperature 23.0 °C
18900 psi
@Temperature 73.4 °F
flatwise; ISO 178
Compressive Strength 220 MPa31900 psiflatwise; ISO 604
Charpy Impact, Notched 3.00 J/cm²14.3 ft-lb/in²Edgewise; IEC 60893-2
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 1.00e+11 ohm1.00e+11 ohmafter immersion in water; IEC 60167
Dielectric Strength 10.0 kV/mm254 kV/inflatwise; IEC 60243-1
Dielectric Breakdown 80000 V80000 VTaper pin electrodes, edgewise; IEC 60243-1
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 µm/m-°C11.1 µin/in-°F
Maximum Service Temperature, Air 155 °C311 °FTemperature Index; IEC 60216
Flammability, UL94 V-0V-0
 
Descriptive Properties
ColorSimilar to Red RAL 3018, Gray RAL 7035, White RAL 9001
ReinforcementChopped glass fibers
Sheet Size (mm)2000 x 1250

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PVONR9924 / 249214

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.