MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Total Lumicene® mPE M 3427 Metallocene Polyethylene, Cast Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Extrusion Grade; LLDPE/Octene, Extruded; LLDPE/Hexene, Molded

Material Notes: Lumicene® mPE M 3427 is a second generation metallocene based Polyethylene with hexene as comonomer.

Lumicene® mPE M 3427 can be processed at high output rates with low extrusion pressure, low neck-in, excellent drawability and good gauge control in comparison with conventional LLDPE and first generation metallocene based polyethylene. The combination of these features combined with excellent optical properties brings a significant downgauging potential.

Lumicene® mPE M 3427 is suited for many applications in the field of consumer, food and hygiene packaging such as hygiene film, stretch wrap (non cling layer) and lamination.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.934 g/cc0.934 g/ccISO 1183
Thickness 20.0 microns0.787 mil
Melt Flow 3.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.1 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 12.0 MPa1740 psiISO 527-3
Film Tensile Strength at Yield, TD 11.5 MPa1670 psiISO 527-3
Film Elongation at Break, MD 480 %480 %ISO 527-3
Film Elongation at Break, TD 590 %590 %ISO 527-3
Elmendorf Tear Strength, MD 2.10 g/micron53.3 g/milISO 6383-2
Elmendorf Tear Strength, TD 11.7 g/micron297 g/milISO 6383-2
Dart Drop Test 53.0 g0.117 lbISO 7765-1
Film Tensile Strength at Break, MD 39.0 MPa5660 psiISO 527-3
Film Tensile Strength at Break, TD 27.0 MPa3920 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 123 °C253 °FISO 11357
Vicat Softening Point 120 °C248 °FISO 306
 
Optical PropertiesMetricEnglishComments
Haze 2.3 %2.3 %ISO 14782
Gloss 86 %86 %at 45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 60.0 °C68.0 - 140 °FChill Roll
Melt Temperature 240 - 280 °C464 - 536 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total Lumicene® mPE M 4707 EP Metallocene Polyethylene, Blown Film
Total Lumicene® mPE M 5220 High Density Polyethylene, Blow Molding
Total Lumicene® mPE M 3509 Medium Density Polyethylene, Blow Molding
Total Lumicene® MR10MX0 Metallocene Random Copolymer Polypropylene, Injection Molding and Injection Blow Molding
Total Lumicene® mPE M 2735 S01 Metallocene Polyethylene, Cast Film

PTOTAL775 / 130500

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.