MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

A. Schulman Diamond Centrex® 601 Profile Extrusion Grade AES  (discontinued **)
Categories: Polymer; Thermoplastic; AES Polymer; AES, Extruded

Material Notes: Centrex 601 resin is a very high-impact, low-gloss AES (acrylonitrile-ethylene-propylene-styrene) resin with good resistance to weather aging. It has good melt strength for profile extrusion and can be coextruded over polyvinyl chloride (PVC).

Applications: Typical applications for Centrex 601 resin include exterior siding and window frames panels. As with any product, use of Centrex 601 resin in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

A. Schulman has acquired Network Polymers & Diamond Polymers.

Key Words: Weatherable Polymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/ccASTM D792
Melt Flow 6.0 g/10 min
@Load 10.0 kg,
Temperature 230 °C
6.0 g/10 min
@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 23.4 MPa3390 psichs 2.0 in/min; ASTM D638
Tensile Strength, Yield 28.3 MPa4100 psichs 2.0 in/min; ASTM D638
Tensile Modulus 1.722 GPa249.8 ksichs 2.0 in/min; ASTM D638
Flexural Strength 44.1 MPa6400 psichs 0.05 in/min; ASTM D790
Flexural Modulus 1.585 GPa229.9 ksitangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched  0.800 J/cm
@Thickness 3.17 mm,
Temperature -40.0 °C
1.50 ft-lb/in
@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
 1.28 J/cm
@Thickness 3.17 mm,
Temperature -18.0 °C
2.40 ft-lb/in
@Thickness 0.125 in,
Temperature -0.400 °F
ASTM D256
 5.34 J/cm
@Thickness 3.17 mm,
Temperature 23.0 °C
10.0 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Impact Test  26.0 J
@Temperature -40.0 °C
19.2 ft-lb
@Temperature -40.0 °F
ASTM D3763
 38.0 J
@Temperature 23.0 °C
28.0 ft-lb
@Temperature 73.4 °F
ASTM D3763
 41.0 J
@Temperature -18.0 °C
30.2 ft-lb
@Temperature -0.400 °F
ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear 28.0 µm/m-°C15.6 µin/in-°FASTM D696
 
Optical PropertiesMetricEnglishComments
Gloss 50 - 70 %50 - 70 %Sheet/Profile; 60°; ASTM D523

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for ASA/AES, Unreinforced, Extruded/Molded
Sax Polymers SAXATEC 6120 AES
A. Schulman Diamond Centrex® 813 General Purpose Injection Molding Grade ASA/AES
Mocom (ALBIS) ALTECH® ABS+PMMA A 1000/500 ABS+PMMA
Polyram RamShine PVS701 AES, UV Stabilized

PDIAM351 / 126442

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.