MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI adhesives

Arkema Oroglas® SG 10 Acrylic, Gamma Radiation Resistant  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Gamma Radiation Resistant, Molded

Material Notes: OROGLAS SG 10 is special Gamma - radiation - resistant formulation designed for use in medical devises.

OROGLAS SG 10 maintains exceptional clarity after 5 megarads of Gamma radiation with no adverse effect on physical properties.

In addition, OROGLAS SG 10 has all the features of oroglas high impact grades including increased flow, clarity and chemical resistance.

OROGLAS SG 10 meets FDA and pharmacopeia XXI class VI toxicity requirements.

ISO data provided by the manufacturer, Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³
Water Absorption 2.0 %2.0 %
Moisture Absorption at Equilibrium 0.36 %0.36 %Humidity Absorption
Melt Flow 2.8 g/10 min
@Load 3.80 kg,
Temperature 230 °C
2.8 g/10 min
@Load 8.38 lb,
Temperature 446 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 42.0 MPa6090 psi50 mm/min
Elongation at Break 30 %30 %Nominal Strain; 50 mm/min
Elongation at Yield 4.5 %4.5 %50 mm/min
Tensile Modulus 1.70 GPa247 ksi1 mm/min
Charpy Impact Unnotched 6.00 J/cm²28.6 ft-lb/in²
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²
Tensile Creep Modulus, 1 hour 1400 MPa203000 psi
Tensile Creep Modulus, 1000 hours 1000 MPa145000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm1.00e+14 ohm
Dielectric Constant  3.2
@Frequency 1e+6 Hz
3.2
@Frequency 1e+6 Hz
 3.9
@Frequency 100 Hz
3.9
@Frequency 100 Hz
Dielectric Strength 15.0 kV/mm381 kV/in
Dissipation Factor  0.040
@Frequency 1e+6 Hz
0.040
@Frequency 1e+6 Hz
 0.050
@Frequency 100 Hz
0.050
@Frequency 100 Hz
Comparative Tracking Index 600 V600 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 100 µm/m-°C
@Temperature 20.0 °C
55.6 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °F
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C178 °F
Vicat Softening Point 84.0 °C183 °F50°C/hr; 50N
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 80 %80 %Mfr. reports 'Transparent' but doesn't quantify.
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Oroglas® SG 7 Acrylic, Gamma Radiation Resistant
INEOS Styrolution Zylar® 960 MBS
Röhm Acrylite® AR Acrylic Sheet, Abrasion Resistant
Covestro Apec® HT KU 1-9357/2 High-Heat Polycarbonate, 20% Glass Fiber
Cossa Polimeri ESTALUX 9202 Methyl Methacrylate Acrylonitrile Butadiene Styrene

PZARKG493 / 25751

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.