MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Coosa Composites Bluewater 20 12 mm Fiberglass Reinforced Polyurethane Foam Panel
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Glass Filled

Material Notes: The Bluewater composite panels are made from high-density closed-cell polyurethane foam reinforced with continuous strand fiberglass and woven roving. They’re used for lightweight building applications that previously called for the use of plywood. The Bluewater series is ideal for projects in marine or high-humidity settings. It is also suitable for applications that require a high strength per cubic foot ratio with the added benefit of being lighter than plywood.

Bluewater 20: The lightest of the three Bluewater options, the Bluewater 20 boasts a density of 20 pounds per cubic foot and is over 45% lighter than plywood. The Bluewater 20 is often used as a semi-structural component and in other non-structural applications. The benefit of the Bluewater 20 is that it is one of the most economical options without compromising on quality and strength.

Information provided by Coosa Composites

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.320 g/cc0.0116 lb/in³ASTM C271
Thickness 12000 microns472 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 2.60 MPa377 psiFlatwise; ASTM C297
Flexural Strength 26.6 MPa3860 psiASTM D790
Flexural Modulus 1.301 GPa188.7 ksiASTM D790
Compressive Strength 3.50 MPa508 psiCore; ASTM C365
Compressive Modulus 0.0631 GPa9.15 ksiCore; ASTM C365
Shear Modulus 0.0251 GPa3.64 ksiCore; ASTM C273
Shear Strength 2.80 MPa406 psiCore; ASTM C273

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOOS903 / 322923

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.