MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

AGC Fluon® TL-120 Micropowder
Categories: Polymer; Thermoplastic; Fluoropolymer; Fluorinated Ethylene Propylene (FEP)

Material Notes: Product Description: Fluon® TL-120 is a white, FEP (fluorinated ethylene propylene) micropowder with a very small particle size. It has excellent thickening power when used as an extreme pressure (EP) agent in hydrocarbon and fluorosilicone fluids, and is used to meet MLGI Class 2 Specifications. Fluon® TL-120 is ideally suited as an additive to all solid and liquid media. In printing inks, it may be used as an anti-scuff and release agent. Fluon® TL-120 is suitable for food contact applications.

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.385 g/cc0.0139 lb/in³ASTM D4894
Volatiles 0.17 %0.17 %
Particle Size 3.0 µm3.0 µmHegman; ASTM D1210
 3.5 µm3.5 µmLow Shear
 14 µm14 µmLow Shear
 34 µm34 µmLow Shear
Specific Surface Area 7.6 m²/g7.6 m²/g
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FASTM D3417
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.10 %<= 0.10 %ASTM D4019
 
Descriptive Properties
Oil Absorption79 lb oil/100 lbASTM D1438
Oil Penetrometer68[1/10 mm], ASTM D1403

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC Fluon® FR 22 PTFE, 10% Graphite Filled
AGC Fluon® FP-EF-101 PTFE, 5% Glass Filled
AGC Fluon® FC168-63 PTFE, 63% Bronze and Graphite Filled
AGC Fluon® FC123 PTFE, 15% Graphite Filled
AGC Fluon® FC100-25 1000 PTFE, 25% Glass Fiber Filled

PAGCX284 / 191393

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.