MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Lucas-Milhaupt Silvaloy® A24 Brazing Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Silvaloy A24 does not contain cadmium and is a lower silver modification to the standard Bag-20 at 30 percent. Its slightly higher melt temperature provides improved mechanical strength when exposed to elevated temperatures or cyclic loads at elevated temperatures. It can be used in joining of copper, brass, nickel, silver, and ferrous alloys. Typical applications are the joining of ferrous, nonferrous and dissimilar metals and alloys with close joint clearances.

Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 8.91 g/cc8.91 g/cc
Density 8.90 g/cc0.322 lb/in³
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000712 ohm-cm0.00000712 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Melting Point 688 - 810 °C1270 - 1490 °F
Solidus 688 °C1270 °F
Liquidus 810 °C1490 °F
Maximum Service Temperature, Air 260 °C500 °Fcontinuous
 371 °C700 °Fintermittent
 
Processing PropertiesMetricEnglishComments
Processing Temperature 816 - 926.1 °C1500 - 1699 °FBrazing Temperature
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 42 - 44 %42 - 44 %
Other, total <= 0.15 %<= 0.15 %
Silver, Ag 23 - 25 %23 - 25 %
Zinc, Zn 31 - 35 %31 - 35 %
 
Descriptive Properties
ColorLight Yellow
Electrical Conductivity (% IACS)24.2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucas-Milhaupt Silvaloy® 255 Brazing Alloy
Silver, Ag
Lucas-Milhaupt Silvacore® A38T Flux Cored Brazing Alloy
Lucas-Milhaupt Easy-Flo 25 Brazing Alloy
Lucas-Milhaupt Silvaloy® A34T Brazing Alloy

NBRW019 / 79795

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.