MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company EMI 161 Z Polypropylene (PP); Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - FDA Compliant Ingredients
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Stainless Fiber, EMI

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.990 g/cc0.990 g/ccASTM D 792
Linear Mold Shrinkage 0.010 cm/cm
@Thickness 3.20 mm
0.010 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 20.7 MPa3000 psiASTM D 638
Elongation at Break >= 10 %>= 10 %ASTM D 638
Tensile Modulus 0.965 GPa140 ksiASTM D 638
Flexural Strength 31.0 MPa4500 psiASTM D 790
Flexural Modulus 1.24 GPa180 ksiASTM D 790
Izod Impact, Notched 2.40 J/cm
@Thickness 3.20 mm
4.50 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
NB
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 10 ohm-cm<= 10 ohm-cmASTM D 257
Surface Resistance <= 10000 ohm<= 10000 ohmESD STM11.11
Surface Resistivity per Square <= 1e+05<= 1e+05ASTM D 257; ESD STM11.11
Static Decay <= 2.0 sec<= 2.0 secFTMS101C; 4046.1
Shielding Effectiveness  46 dB
@Thickness 2.00 mm,
Frequency 1e+9 Hz
46 dB
@Thickness 0.0787 in,
Frequency 1e+9 Hz
ASTM D 4935
 46 dB
@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
46 dB
@Thickness 0.0787 in,
Frequency 1.30e+9 Hz
ASTM D 4935
 46 dB
@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
46 dB
@Thickness 0.0787 in,
Frequency 7.00e+8 Hz
ASTM D 4935
 47 dB
@Thickness 2.00 mm,
Frequency 5.00e+8 Hz
47 dB
@Thickness 0.0787 in,
Frequency 5.00e+8 Hz
ASTM D 4935
 48 dB
@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
48 dB
@Thickness 0.0787 in,
Frequency 1.50e+9 Hz
ASTM D 4935
 53 dB
@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
53 dB
@Thickness 0.0787 in,
Frequency 3.00e+8 Hz
ASTM D 4935
 58 dB
@Thickness 3.00 mm,
Frequency 3.00e+8 Hz
58 dB
@Thickness 0.118 in,
Frequency 3.00e+8 Hz
ASTM D 4935
 61 dB
@Thickness 3.00 mm,
Frequency 5.00e+8 Hz
61 dB
@Thickness 0.118 in,
Frequency 5.00e+8 Hz
ASTM D 4935
 63 dB
@Thickness 3.00 mm,
Frequency 7.00e+8 Hz
63 dB
@Thickness 0.118 in,
Frequency 7.00e+8 Hz
ASTM D 4935
 64 dB
@Thickness 3.00 mm,
Frequency 1e+9 Hz
64 dB
@Thickness 0.118 in,
Frequency 1e+9 Hz
ASTM D 4935
 68 dB
@Thickness 3.00 mm,
Frequency 1.30e+9 Hz
68 dB
@Thickness 0.118 in,
Frequency 1.30e+9 Hz
ASTM D 4935
 70 dB
@Thickness 3.00 mm,
Frequency 1.50e+9 Hz
70 dB
@Thickness 0.118 in,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 193 - 221 °C380 - 430 °F
Mold Temperature 37.8 - 51.7 °C100 - 125 °F
Drying Temperature 79.4 °C
@Time 7200 sec
175 °F
@Time 2.00 hour
Moisture Content 0.10 %0.10 %
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 128 HI Z  Polypropylene (PP) Talc 20% - High Impact - FDA Type
RheTech Products GC20P105-08FA 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, FDA Compliant, Black
RTP Company RTP 103 Z Polypropylene (PP), Glass Fiber - FDA Compliant Ingredients
LG Chemical LUPOL GP2200 PP+GF20%
Amco PRIMATOP PP HOMO 201NA Injection Molding Polypropylene

PQZUA4171 / 134884

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.