MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Syensqo (Solvay Specialty Polymers) Veradel® AG-320 Polyethersulfone (PESU), 20% glass fiber
Categories: Polymer; Thermoplastic; Polyethersulfone (PES); Polyethersulfone (PES), 10%Glass Fiber Filled

Material Notes: 20% glass fiber, opaque, high melt flow for injection molding

Veradel® AG-320 is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resistance of the material, while maintaining most of its other basic characteristics. The combination of structural properties and cost effectiveness make this resin an attractive alternative to metals in many engineering applications.

This grade was formerly marketed as Radel® A PESU

- Natural: Veradel® AG-320 NT
- Black: Veradel® AG-320 BK 184

Markets/Uses: Automotive / Automotive E/E / Engine Sensors; Automotive / Automotive E/E / Sensors

Applications: Appliance Components; Appliances; Automotive Electronics; Batteries; Business Equipment; Electrical Parts; Electrical/Electronic Applications; Food Service Applications; Industrial Applications; Metal Replacement; Microwave Cookware; Plumbing Parts; Valves/Valve Parts

Features: Acid Resistant; Chemical Resistant; Creep Resistant; Flame Retardant; Food Contact Acceptable; Good Adhesion; Good Dimensional Stability; Good Strength; Good Thermal Stability; Good Toughness; High Heat Resistance; High Rigidity; High Tensile Strength; Hydrolysis Resistant; Medium Flow; Medium Molecular Weight

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³ASTM D792
Water Absorption 0.45 %
@Time 86400 sec
0.45 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inASTM D955
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 343 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 649 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 109 MPa15800 psiASTM D638
Elongation at Break 3.2 %3.2 %ASTM D638
Tensile Modulus 5.69 GPa825 ksiASTM D638
Flexural Strength 162 MPa23500 psiASTM D790
Flexural Modulus 6.55 GPa950 ksiASTM D790
Izod Impact, Notched 0.590 J/cm1.11 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmASTM D257
Dielectric Constant  3.84
@Frequency 1000 Hz
3.84
@Frequency 1000 Hz
ASTM D150
 3.84
@Frequency 60 Hz
3.84
@Frequency 60 Hz
ASTM D150
 3.88
@Frequency 1e+6 Hz
3.88
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm432 kV/inASTM D149
Dissipation Factor  0.0015
@Frequency 60 Hz
0.0015
@Frequency 60 Hz
ASTM D150
 0.0018
@Frequency 1000 Hz
0.0018
@Frequency 1000 Hz
ASTM D150
 0.0081
@Frequency 1e+6 Hz
0.0081
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 120 - 179 sec120 - 179 secASTM D495
 120 - 179 sec120 - 179 secPLC 5; ASTM D495
Comparative Tracking Index 100 - 174 V100 - 174 VPLC 4; UL 746
 100 - 250 V100 - 250 VUL 746
Hot Wire Ignition, HWI 30 - 59 sec30 - 59 secPLC 2; UL 746
 60 - 119 sec60 - 119 secPLC 1; UL 746
 51 sec
@Thickness 0.400 mm
51 sec
@Thickness 0.0157 in
UL 746
 67 sec
@Thickness 0.800 mm
67 sec
@Thickness 0.0315 in
UL 746
High Amp Arc Ignition, HAI >= 120 arcs>= 120 arcsPLC 0; UL 746
 >= 120 arcs
@Thickness 0.400 mm
>= 120 arcs
@Thickness 0.0157 in
UL 746
 >= 120 arcs
@Thickness 0.800 mm
>= 120 arcs
@Thickness 0.0315 in
UL 746
 >= 120 arcs
@Thickness 3.00 mm
>= 120 arcs
@Thickness 0.118 in
UL 746
High Voltage Arc-Tracking Rate, HVTR 80.1 - 150 mm/min3.15 - 5.91 in/minUL 746
 80.1 - 150 mm/min3.15 - 5.91 in/minPLC 3; UL 746
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 31.0 µm/m-°C
@Thickness 3.18 mm
17.2 µin/in-°F
@Thickness 0.125 in
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 214 °C
@Thickness 3.18 mm
417 °F
@Thickness 0.125 in
Unannealed; ASTM D648
UL RTI, Electrical 180 °C
@Thickness 0.430 mm
356 °F
@Thickness 0.0169 in
UL RTI, Mechanical with Impact 180 °C
@Thickness 0.430 mm
356 °F
@Thickness 0.0169 in
UL RTI, Mechanical without Impact 180 °C
@Thickness 0.430 mm
356 °F
@Thickness 0.0169 in
Flammability, UL94 V-0
@Thickness 0.430 mm
V-0
@Thickness 0.0169 in
Glow Wire Ignition Temperature 850 °C
@Thickness 0.430 mm
1560 °F
@Thickness 0.0169 in
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 0.430 mm
1760 °F
@Thickness 0.0169 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 343 - 399 °C649 - 750 °FInjection
Mold Temperature 149 - 163 °C300 - 325 °F
Drying Temperature 149 - 177 °C
@Time 9000 - 14400 sec
300 - 351 °F
@Time 2.50 - 4.00 hour
Back Pressure 0.345 - 0.689 MPa50.0 - 99.9 psi
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack; Colors Available; Natural Color
FormsPellets
Injection RateFast
ProcessingInjection Molding
RoHS ComplianceYes
Screw Compression Ratio2.0:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4609 / 280409

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.