MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Unitemp 1753 Nickel Superalloy (AF 1753)
Categories: Metal; Superalloy; Nickel Base

Material Notes: Typical Applications: Gas turbine parts, blades, discs, rings, spacers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.45 g/cc0.305 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  44.8 MPa
@Temperature 982 °C,
Time 3.60e+6 sec
6500 psi
@Temperature 1800 °F,
Time 1000 hour
 68.9 MPa
@Temperature 982 °C,
Time 360000 sec
10000 psi
@Temperature 1800 °F,
Time 100 hour
 234 MPa
@Temperature 816 °C,
Time 3.60e+6 sec
34000 psi
@Temperature 1500 °F,
Time 1000 hour
 324 MPa
@Temperature 816 °C,
Time 360000 sec
47000 psi
@Temperature 1500 °F,
Time 100 hour
 676 MPa
@Temperature 649 °C,
Time 3.60e+6 sec
98000 psi
@Temperature 1200 °F,
Time 1000 hour
 793 MPa
@Temperature 649 °C,
Time 360000 sec
115000 psi
@Temperature 1200 °F,
Time 100 hour
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 1.9 %1.9 %
Boron, B 0.0080 %0.0080 %
Carbon, C 0.24 %0.24 %
Chromium, Cr 16.25 %16.25 %
Cobalt, Co 7.2 %7.2 %
Iron, Fe 9.5 %9.5 %
Manganese, Mn 0.050 %0.050 %
Nickel, Ni 53.092 %53.092 %As Balance
Silicon, Si 0.10 %0.10 %
Titanium, Ti 3.2 %3.2 %
Tungsten, W 8.4 %8.4 %
Zirconium, Zr 0.060 %0.060 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allvac® 718Plus™ Nickel Superalloy
Molybdenum, Mo, Annealed
301 Stainless Steel
ATI Allvac® Nickelvac® 606 Nickel Superalloy
Kennametal Stellite Nistelle Super C Nickel Superalloy

NZ97046 / 191445

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.