PRE-ELEC® PP 1393 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity, PRE-ELEC® PP 1393 has an excellent balance of mechanical properties and it is easy to process. Applications: Injection moulded parts for the automotive, medical and electronics industries where a very low volume resistivity is needed. PRE-ELEC® PP 1393 can also be used as a masterbatch and blended with PP. It can also be used in extrusion applications. Processing: PRE-ELEC® PP 1393 compound can be extruded and injection moulded with machines using normal processing conditions as with polypropylene. Test Specimen: 10[mm] wide moulded rod Information from Premix OY |