MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

3M Scotchkote™ UV 840 Urethane Coating
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Liquid

Material Notes: Scotchkote Urethane Coating UV 840 has been developed to provide a durable gloss finish for use as the final coat of 3M coating systems in the construction and transport industries, where an ease of removal of graffiti is required.

Product Features:

  • Combines good application characteristics with excellent gloss and color retention
  • Suitable for use in corrosion protection applications
  • Good resistance to abrasion and mechanical damage
  • Excellent adhesion on correctly prepared and primed surfaces
  • The fully cured coating offers excellent resistance to aqueous solutions, oils, fats and a wide range of industrial chemicals
  • Dry service temperature range up to 100°C

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 55 %55 %
Volatile Organic Compounds (VOC) Content 425 - 485 g/l425 - 485 g/ldepending on color
Thickness 1020 microns40.0 milDry
 1830 microns72.0 milWet
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 100 °C212 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 180 - 240 min3.00 - 4.00 hourTouch Dry
 960 min16.0 hourHard Dry
 10100 min168 hourFull Cure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35292 / 170039

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.