  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Spartech Royalite R59M Hi-Impact ABS/PVC Resin
Categories: Polymer; Thermoplastic; ABS Polymer; ABS/PVC Alloy; Vinyl (PVC)

Material Notes: Data provided by the manufacturer. A unique ABS/PVC resin that meets the flammability standards of many industries and is a cost-effective alternative to standard fire-rated ABS. High rigidity in thin sections and consistent, high-quality color and gloss make it ideal for computer housings

Key Words: Poly(Acrylonitrile-Butadiene-Styrene); Polyvinyl Chloride
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ASTM D792
Water Absorption 0.020 %0.020 %24 hrs. ASTM D570
Viscosity 190400 cP
@Shear Rate 3000 1/s,
Temperature 191 °C
190400 cP
@Shear Rate 3000 1/s,
Temperature 375 °F
Melt Viscosity
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inASTM D955
Melt Flow 1.8 g/10 min
@Load 5.00 kg,
Temperature 200 °C
1.8 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Condition G; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8383ASTM D785
Tensile Strength, Yield 37.6 MPa5450 psiASTM D638
Modulus of Elasticity 1.80 GPa261 ksiASTM D638
Flexural Yield Strength 57.5 MPa8340 psiASTM D790
Flexural Modulus 2.10 GPa305 ksiASTM D790
Izod Impact, Notched 7.40 J/cm13.9 ft-lb/inASTM D256
 1.30 J/cm
@Temperature -20.0 °C
2.44 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 155 µm/m-°C
@Temperature 20.0 °C
86.1 µin/in-°F
@Temperature 68.0 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C207 °FAnnealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C178 °FAnnealed; ASTM D648
Vicat Softening Point 80.0 °C176 °FASTM D1525
Flammability, UL94 5VA
@Thickness 2.16 mm
5VA
@Thickness 0.0850 in
Oxygen Index 29.9 %29.9 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Novatec Novaloy® 9000 PVC + ABS
Spartech Royalite R60M Hi-Impact ABS/PVC Resin
SEKISUI SPI KYDEX® 410 ABS/PVC
Overview of materials for PVC, Molded
Overview of materials for ABS/PVC Alloy

PROY33 / 66393

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.