MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LyondellBasell Petrothene GA643962 Linear Medium Density Polyethylene (LMDPE), Rotational Molded
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Linear Medium Density Polyethylene (LMDPE), Rotational Molded

Material Notes: Petrothene GA643962 is a linear medium density polyethylene selected for rotomolding a variety of objects, including drums, agricultural and chemical storage containers, playground equipment and municipal trash containers. GA643962 is UV-stabilized and is also available in 35-mesh powder as Microthene MP643962. Applications: Containers, Drums, Intermediate Bulk Containers, Jerry Cans, Sports, Leisure & Toys

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.9395 g/cc0.03394 lb/in³ASTM D1505
ESCR 100% Igepal® >= 1000 hour>= 1000 hourCond. A; ASTM D 1693
Melt Flow 3.6 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.6 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 20.0 MPa2900 psiASTM D638
Flexural Modulus, 1% Secant 820 MPa119000 psiASTM D790
2% Secant Modulus 0.700 GPa102 ksiASTM D790
Impact Test  55.0 J
@Temperature -40.0 °C
40.6 ft-lb
@Temperature -40.0 °F
1/4" specimen, ARM
 215 J
@Temperature -40.0 °C
159 ft-lb
@Temperature -40.0 °F
1/4" specimen, ARM
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 40.0 °C104 °Funannealed; ASTM D648
 58.0 °C136 °Funannealed; ASTM D648
 
Descriptive Properties
Processing MethodRotomolding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Rotational Molded
Nexeo® HIVAL® 106033 Linear Low Density Polyethylene
Nexeo® HIVAL® 103538 Linear Low Density Polyethylene
ICO Polymers ICORENE™ 110-1328 LMDPE Rotational Molding Resin

PEQT8831 / 220465

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.