MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

NOVA Chemicals Sclair® 14B3 Butene LMDPE Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Linear Medium Density Polyethylene (LMDPE), Film

Material Notes: Film Properties. Features: Low gel, good clarity, heat resistance and barrier properties.

Applications: Lamination, co-extrusion.

Data provided by the manufacturer.

Key Words: Linear Medium Density Polyethylene; Polybutene; Polyolefin
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.936 g/cc0.0338 lb/in³ASTM D792
Melt Flow 1.8 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.8 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 17.0 MPa2470 psiASTM D882
Film Tensile Strength at Yield, TD 18.0 MPa2610 psiASTM D882
Film Elongation at Break, MD 750 %750 %ASTM D882
Film Elongation at Break, TD 950 %950 %ASTM D882
Secant Modulus, MD 0.340 GPa49.3 ksiASTM D882
Secant Modulus, TD 0.370 GPa53.7 ksiASTM D882
Coefficient of Friction 0.400.40ASTM D1894
Elmendorf Tear Strength, MD 1.00 g/micron25.4 g/milASTM D1922
Elmendorf Tear Strength, TD 5.00 g/micron127 g/milASTM D1922
Dart Drop 1.00 g/micron25.4 g/milF 50; ASTM D1709/A
Film Tensile Strength at Break, MD 42.0 MPa6090 psiASTM D882
Film Tensile Strength at Break, TD 38.0 MPa5510 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 111 °C232 °FASTM D1525
Brittleness Temperature <= -70.0 °C<= -94.0 °FASTM D696
 
Optical PropertiesMetricEnglishComments
Haze 15 %
@Thickness 0.0250 mm
15 %
@Thickness 0.000984 in
ASTM D1003
Gloss 58 %58 %45°; 1 mil; ASTM D1894
 
Processing PropertiesMetricEnglishComments
Melt Temperature 225 - 235 °C437 - 455 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEHN0L / 35534

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.