MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LyondellBasell Adflex™ Q 402 F Polyolefin
Categories: Polymer; Film; Thermoplastic; Polyolefin; Polyolefin, Film Grade; Polyolefin, Film Grade (Polyolefin)

Material Notes: Description: Adflex™ Q 402 F thermoplastic olefin resin is designed for air quenched blown film applications. Q 402 F resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, except for certain fatty foods. All ingredients meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Film property values shown were determined on 2.0 mil thickness blown film extruded at 460°F, 2.5:1 BUR, with a 80 mil die gap. Uses: Film, heavy duty bags, packaging

Information provided by Basell.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.892 g/cc0.0322 lb/in³ASTM D792
Thickness 50.8 microns2.00 mil
Melt Flow 0.65 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.65 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 17.9 MPa2600 psiASTM D882
Film Tensile Strength at Yield, TD 15.2 MPa2200 psiASTM D882
Film Elongation at Break, MD 670 %670 %ASTM D882
Film Elongation at Break, TD 870 %870 %ASTM D882
Secant Modulus, MD 0.330 GPa47.9 ksi2% Secant, 2 mil; ASTM D882
Secant Modulus, TD 0.303 GPa43.9 ksi2% Secant, 2 mil; ASTM D882
Elmendorf Tear Strength, MD 8.66 g/micron220 g/milMethod A; ASTM D1922
Elmendorf Tear Strength, TD 18.1 g/micron460 g/milMethod A; ASTM D1922
Dart Drop 10.8 g/micron275 g/milMethod A; ASTM D1709
Film Tensile Strength at Break, MD 68.3 MPa9900 psiASTM D882
Film Tensile Strength at Break, TD 48.3 MPa7000 psiASTM D882
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Heat Resistance305°FBasell Test Method
Puncture Resistance160 ft-lb/in3Basell Test Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Adflex™ Q 100 F Polyolefin
LyondellBasell Adflex™ Q 200 F Polyolefin
LyondellBasell Adflex™ KS-021P TPO Resin
LyondellBasell Astryn 65F5-4 Polypropylene Homopolymer, 40% Calcium Carbonate
LyondellBasell Astryn 65F4-4 Polypropylene Homopolymer, 40% Talc

PMO760 / 53749

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.