MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Versalis Clearflex® RM 50 U Linear Medium Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Linear Medium Density Polyethylene (LMDPE), Rotational Molded

Material Notes: Clearflex RM 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.

Items manufactured with Clearflex RM 50 U show good mechanical properties and high environmental stress crack resistance (ESCR).

Main Applications: Thanks to good balance between mechanical properties and processability, Clearflex RM 50 U is recommended for the production of medium capacity containers and items with difficult shapes.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.936 g/cc0.936 g/ccISO 1183
Environmental Stress Crack Resistance >= 350 hour>= 350 hourISO 22088
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5454ISO 868/A
Tensile Strength at Break 21.0 MPa3050 psiISO 527
Tensile Strength, Yield 18.0 MPa2610 psiISO 527
Elongation at Break >= 700 %>= 700 %ISO 527
Flexural Modulus 0.690 GPa100 ksiISO 178
Dart Drop Total Energy 220 J/cm0.412 ft-lb/milrotomolded sample; ISO 6603/2
 
Thermal PropertiesMetricEnglishComments
Melting Point 126 °C259 °FInternal method
Vicat Softening Point 114 °C
@Load 1.00 kg
237 °F
@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -70.0 °C<= -94.0 °FASTM D746
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %clear; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polimeros Mexicanos Rotolene® 93835-TG Medium Density Polyethylene
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Rotational Molded
Polimeros Mexicanos Rotolene® 93050 Medium Density Polyethylene
Polimeros Mexicanos Rotolene® Black Plus Polyethylene
Overview of materials for High Density Polyethylene (HDPE), Rotational Molding Grade

PENG080 / 124474

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.