MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Northstar Polymers MGB-A80AQ High Performance Polyurethane Cast Elastomer System 80A
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Liquid

Material Notes: This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires high rebound, slide abrasion, constant water contact and high elongation. Possible applications for this material include roller skate wheels, bumpers, abrasion resistant liners, rock/sand sizing screens and other specialty applications. Unlike conventional full-prepolymer systems, quasi system formulation improves processability, in-mold flow, and components mixing by use of low viscosity prepolymer. This results better physical properties of the products. Can be approved for FDA dry food contact.

Information provided by Northstar Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ASTM D2240
Tensile Strength 25.67 MPa3723 psiASTM D412
Elongation at Break 554 %554 %ASTM D412
Rebound 63 %63 %Bashore Rebound; ASTM D2632
Tear Strength 22.8 kN/m130 pliSplit; ASTM D624
 71.9 kN/m410 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 2020ASTM D4060
 
Processing PropertiesMetricEnglishComments
Processing Temperature 25.0 °C77.0 °FCuring Agent Temperature
 82.2 - 93.3 °C180 - 200 °FPrepolymer Temperature
Mold Temperature 82.2 - 93.3 °C180 - 200 °F
Cure Time  30.0 min
@Temperature 93.3 °C
0.500 hour
@Temperature 200 °F
De-mold Time
 960 min
@Temperature 82.2 °C
16.0 hour
@Temperature 180 °F
Complete Cure Cycle
Pot Life 2.50 - 3.00 min2.50 - 3.00 min
 
Descriptive Properties
Curing AgentGBA-042
PrepolymerMGA-018
Weight Ratio1:2.232Prepolymer to Curing Agent Ratio

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Non-Black Sulfur Cure
Northstar Polymers MSS-A80AQ High Performance Polyurethane Cast Elastomer System 80A
Covestro DESMODUR® TTX134 + BAYTEC® XL 1705, 80A Polyurethane, TDI- PTMEG
Covestro DESMODUR® MT2173 + BAYTEC® T20 + BAYTEC® XL B (D1-2 catalyst), 80A Polyurethane, MDI- PTMEG

PNORTH01 / 54836

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.