Applications include edge tools, wear-resistant parts, high-stress flat springs, hot coiled springs, plow beams, plow shares, scraper blades, discs, mower knives, and harrow teeth. Post oil quenched hardness: 40 HRC surface, 37 HRC half-radius, 30 HRC center |
UNS G10950, AMS 5121, AMS 5122, AMS 5132, AMS 7304, ASTM A29, ASTM A510, ASTM A576, ASTM A682, FED QQ-S-700 (C1095), MIL SPEC MIL-S-16788 (C10), SAE J403, SAE J412, SAE J414, DIN 1.1274, JIS SUP 4, SS14 1870 (Sweden), B.S. 060 A 96, B.S. EN 44 B |