Envalior Pocan® B 1505 Z 000000 PBT
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), Extrusion Grade
;
Polybutylene Terephthalate (PBT), Impact Grade
;
Polybutylene Terephthalate (PBT), Unreinforced, Molded
Material Notes:
PBT, non-reinforced, injection molding, extrusion, impact modified
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.29
g/cc
0.0466
lb/in³
ISO 1183
Melt Flow
26
g/10 min
@Load 2.16 kg,
Temperature 260 °C
26
g/10 min
@Load 4.76 lb,
Temperature 500 °F
Estimated using room temperature density; ISO 1133
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
52.0
MPa
7540
psi
ISO 527-1/-2
Elongation at Break
50 %
50 %
Nominal; ISO 527-1/-2
Elongation at Yield
4.2 %
4.2 %
ISO 527-1/-2
Tensile Modulus
2.40
GPa
348
ksi
ISO 527-1/-2
Charpy Impact Unnotched
22.0
J/cm²
@Temperature -30.0 °C
105
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
105
µm/m-°C
58.3
µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow
105
µm/m-°C
58.3
µin/in-°F
ISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi)
120
°C
248
°F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi)
55.0
°C
131
°F
ISO 75-1/-2
Processing Properties
Metric
English
Comments
Melt Temperature
260
°C
500
°F
Injection Molding; ISO 294
Mold Temperature
80.0
°C
176
°F
Injection Molding; ISO 10724
Descriptive Properties
Additives
Lubricants
Release agent
Features
Heat stabilized or stable to heat
High impact or high impact modified
Form
Pellets
ISO Short Name
ISO 7792-1-PBT,GHMPR,11-020
Processing
Injection molding
Region
Asia Pacific
Europe
Near East/Africa
North America
South and Central America
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Envalior Pocan® B 1505 000000 PBT
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Evonik Vestodur® HI19 Polymer Modified PBT
Envalior Pocan® B 1600 000000 PBT
Envalior Pocan® B 1100 000000 PBT
PLANX0845 / 99060
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.