MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

AISI Type S45500 Stainless Steel, annealed at 815°C (1500°F) for 30 minutes, water quenched, bar
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T S40000 Series Stainless Steel

Material Notes: Martensitic, age-hardenable, easily formable (annealed), no corrosion in fresh water, resists staining in normal air atmosphere, good resistance to pitting in 5% salt spray and 5% ferric chloride. For use in service temperatures up to 425°C.

Key Words: UNS S45500, AMS 5578, AMS 5617, AMS 5672, AMS 5860, ASTM A313 (XM-16), ASTM A564 (XM-16), ASTM A705 (XM-16), martensitic, pitting resistant, T S45500
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell  297
@Diameter 25.4 mm
297
@Diameter 1.00 in
Converted from Rockwell C hardness.
 297
@Diameter 102 mm
297
@Diameter 4.00 in
Converted from Rockwell C hardness.
Hardness, Knoop  318
@Diameter 25.4 mm
318
@Diameter 1.00 in
Converted from Rockwell C hardness.
 318
@Diameter 102 mm
318
@Diameter 4.00 in
Converted from Rockwell C hardness.
Hardness, Rockwell C  31
@Diameter 25.4 mm
31
@Diameter 1.00 in
 31
@Diameter 102 mm
31
@Diameter 4.00 in
Hardness, Vickers  308
@Diameter 25.4 mm
308
@Diameter 1.00 in
Converted from Rockwell C hardness.
 308
@Diameter 102 mm
308
@Diameter 4.00 in
Converted from Rockwell C hardness.
Tensile Strength, Ultimate  965 MPa
@Diameter 102 mm
140000 psi
@Diameter 4.00 in
 1000 MPa
@Diameter 25.4 mm
145000 psi
@Diameter 1.00 in
Tensile Strength, Yield  795 MPa
@Strain 0.2 %,
Diameter 25.4 mm
115000 psi
@Strain 0.2 %,
Diameter 1.00 in
 795 MPa
@Strain 0.2 %,
Diameter 102 mm
115000 psi
@Strain 0.2 %,
Diameter 4.00 in
Elongation at Break  12 %
@Diameter 102 mm
12 %
@Diameter 4.00 in
in 50 mm
 14 %
@Diameter 25.4 mm
14 %
@Diameter 1.00 in
in 50 mm
Modulus of Elasticity 200 GPa29000 ksiTypical for stainless steel
Notched Tensile Strength 1585 MPa
@Diameter 25.4 mm
229900 psi
@Diameter 1.00 in
Charpy Impact 95.0 J
@Diameter 25.4 mm
70.1 ft-lb
@Diameter 1.00 in
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000900 ohm-cm0.0000900 ohm-cmannealed, 0.000075 Ohm-cm when annealed and aged at 510°C for 4 hours and air cooled.
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.1 µm/m-°C
@Temperature 24.0 - 150 °C
5.61 µin/in-°F
@Temperature 75.2 - 302 °F
when annealed at 1040°C, water quenched
 10.3 µm/m-°C
@Temperature 24.0 - 205 °C
5.72 µin/in-°F
@Temperature 75.2 - 401 °F
when annealed at 1040°C, water quenched
 10.6 µm/m-°C
@Temperature 24.0 - 95.0 °C
5.89 µin/in-°F
@Temperature 75.2 - 203 °F
 10.6 µm/m-°C
@Temperature 24.0 - 205 °C
5.89 µin/in-°F
@Temperature 75.2 - 401 °F
when annealed and aged at 480°C for 4 hours, air cooled
 10.8 µm/m-°C
@Temperature 24.0 - 95.0 °C
6.00 µin/in-°F
@Temperature 75.2 - 203 °F
when annealed and aged at 480°C for 4 hours, air cooled
 11.7 µm/m-°C
@Temperature 22.0 - 260 °C
6.50 µin/in-°F
@Temperature 71.6 - 500 °F
 12.1 µm/m-°C
@Temperature 22.0 - 315 °C
6.72 µin/in-°F
@Temperature 71.6 - 599 °F
Specific Heat Capacity 0.480 J/g-°C0.115 BTU/lb-°FTypical value for stainless steel.
Thermal Conductivity  18.0 W/m-K
@Temperature 100 °C
125 BTU-in/hr-ft²-°F
@Temperature 212 °F
 19.7 W/m-K
@Temperature 200 °C
137 BTU-in/hr-ft²-°F
@Temperature 392 °F
 21.3 W/m-K
@Temperature 300 °C
148 BTU-in/hr-ft²-°F
@Temperature 572 °F
 23.4 W/m-K
@Temperature 400 °C
162 BTU-in/hr-ft²-°F
@Temperature 752 °F
 24.7 W/m-K
@Temperature 500 °C
171 BTU-in/hr-ft²-°F
@Temperature 932 °F
Maximum Service Temperature, Air 425 °C797 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.050 %<= 0.050 %
Chromium, Cr 11.8 %11.8 %
Copper, Cu 2.0 %2.0 %
Iron, Fe 73 %73 %
Manganese, Mn <= 0.50 %<= 0.50 %
Molybdenum, Mo <= 0.50 %<= 0.50 %
Nickel, Ni 8.5 %8.5 %
Niobium, Nb (Columbium, Cb) 2.0 %2.0 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 0.50 %<= 0.50 %
Sulfur, S <= 0.030 %<= 0.030 %
Titanium, Ti 1.1 %1.1 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type S45500 Stainless Steel, hardened at 480°C (900°F) for 4 hours, air cooled
AISI Type S45500 Stainless Steel, hardened at 815°C (1500°F) for 30 minutes, water quenched, aged at 480°C (900°F) for 4 hours
Haynes Hastelloy® B-3® alloy, 0% cold work
AISI Type 450 Stainless Steel, 25 mm diameter bar, solution annealed
Sandvik Ti Grade 9 Tube and pipe, seamless

MQM455A / 13834

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.