MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company EMI 663 Acrylonitrile Butadiene Styrene (ABS) Stainless Steel Fiber - EMI/RFI Shielding
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D 792
Additive Loading 20 %20 %Primary Additive
Linear Mold Shrinkage 0.0030 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0030 - 0.0080 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 29.0 MPa4200 psiASTM D 638
Elongation at Break 2.0 %2.0 %ASTM D 638
Tensile Modulus 2.76 GPa400 ksiASTM D 638
Flexural Strength 53.1 MPa7700 psiASTM D 790
Flexural Modulus 2.96 GPa430 ksiASTM D 790
Izod Impact, Notched 0.534 J/cm
@Thickness 3.20 mm
1.00 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 1.28 J/cm
@Thickness 3.20 mm
2.40 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.10 ohm-cm<= 0.10 ohm-cmASTM D 257
Surface Resistance <= 1000 ohm<= 1000 ohmESD STM11.11
Surface Resistivity per Square <= 10000 ohm<= 10000 ohmASTM D 257; ESD STM11.11
Static Decay <= 0.50 sec<= 0.50 secFTMS101C; 4046.1
Shielding Effectiveness  98 dB
@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
98 dB
@Thickness 0.0787 in,
Frequency 3.00e+8 Hz
ASTM D 4935
 102 dB
@Thickness 2.00 mm,
Frequency 5.00e+8 Hz
102 dB
@Thickness 0.0787 in,
Frequency 5.00e+8 Hz
ASTM D 4935
 105 dB
@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
105 dB
@Thickness 0.0787 in,
Frequency 7.00e+8 Hz
ASTM D 4935
 108 dB
@Thickness 2.00 mm,
Frequency 1e+9 Hz
108 dB
@Thickness 0.0787 in,
Frequency 1e+9 Hz
ASTM D 4935
 108 dB
@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
108 dB
@Thickness 0.0787 in,
Frequency 1.30e+9 Hz
ASTM D 4935
 108 dB
@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
108 dB
@Thickness 0.0787 in,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 - 246 °C400 - 475 °F
Mold Temperature 65.6 - 82.2 °C150 - 180 °F
Drying Temperature 82.2 °C
@Time 7200 sec
180 °F
@Time 2.00 hour
Moisture Content 0.10 %0.10 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 2286 HF TFE 15  Polyetheretherketone (PEEK) Carbon Fiber 35% - PTFE 15% - High Flow
RTP Company RTP 1083 HEC FR Polybutylene Terephthalate (PBT), Electrically Conductive - EMI/RFI Shielding - Nickel-Coated Carbon Fiber - Flame Retardant
RTP Company RTP 283 D TFE 15 Nylon 6/12 (PA), Carbon Fiber - PTFE Lubricated
RTP Company RTP 2799S X 89622 C  Styrenic Thermoplastic Elastomer (TES) Thermally Conductive - Electrically Conductive - SEBS
RTP Company RTP 2799 S X 91655 BLACK Saturated Styrenic Block Copolymer

PQZVA17456 / 120443

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.