MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Honeywell UltRx 400 CTFE Homopolymer, Barrier Film
Categories: Polymer; Film; Thermoplastic; Fluoropolymer; Polychlorotrifluoroethylene (PCTFE); Molded

Material Notes: Aclar® UltRx 4000 film is a 4.00 mil (102 micron) PCTFE homopolymer, high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipment and provides the highest barrier of any clear film.

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.11 g/cc
@Thickness 0.102 mm
0.0762 lb/in³
@Thickness 0.00400 in
50% RH; ASTM D1505
Water Vapor Transmission  0.00900 g/m²/day
@Temperature 25.0 °C
0.000580 g/100 in²/day
@Temperature 77.0 °F
60% RH; ASTM F1249
 0.0150 g/m²/day
@Temperature 30.0 °C
0.000966 g/100 in²/day
@Temperature 86.0 °F
65% RH; ASTM F1249
 0.0160 g/m²/day
@Temperature 30.0 °C
0.00103 g/100 in²/day
@Temperature 86.0 °F
60% RH; ASTM F1249
 0.0480 g/m²/day
@Temperature 40.0 °C
0.00309 g/100 in²/day
@Temperature 104 °F
75% RH; ASTM F1249
 0.0650 g/m²/day
@Temperature 37.8 °C
0.00419 g/100 in²/day
@Temperature 100 °F
100% RH; ASTM F1249
Surface Tension >= 42 dynes/cm
@Thickness 0.102 mm
>= 42 dynes/cm
@Thickness 0.00400 in
50% RH, treated side; ASTM D2578
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 150 - 225 %
@Thickness 0.102 mm
150 - 225 %
@Thickness 0.00400 in
50% RH; ASTM D882
Film Elongation at Break, TD 175 - 225 %
@Thickness 0.102 mm
175 - 225 %
@Thickness 0.00400 in
50% RH; ASTM D882
Secant Modulus, MD 1.103 - 1.379 GPa
@Thickness 0.102 mm
160.0 - 200.0 ksi
@Thickness 0.00400 in
50% RH; ASTM D882
Secant Modulus, TD 1.103 - 1.379 GPa
@Thickness 0.102 mm
160.0 - 200.0 ksi
@Thickness 0.00400 in
50% RH; ASTM D882
Film Tensile Strength at Break, MD 41.0 - 62.0 MPa
@Thickness 0.102 mm
5950 - 8990 psi
@Thickness 0.00400 in
50% RH; ASTM D882
Film Tensile Strength at Break, TD 28.0 - 48.0 MPa
@Thickness 0.102 mm
4060 - 6960 psi
@Thickness 0.00400 in
50% RH; ASTM D882
 
Thermal PropertiesMetricEnglishComments
Crystallization Temperature 211 °C
@Thickness 0.00400 mm
412 °F
@Thickness 0.000157 in
Melting, 50% RH; ASTM D4591
Shrinkage, MD <= 5.0 %
@Temperature 149 °C,
Time Error in fixSigDigits: @digits must be between 1 a sec
<= 5.0 %
@Temperature 300 °F,
Time Error in fixSigDigits: @digits must be between 1 a hour
4 mil, 50% RH; ASMT D1204
Shrinkage, TD <= -5.00 %
@Temperature 149 °C,
Time Error in fixSigDigits: @digits must be between 1 a sec
<= -5.00 %
@Temperature 300 °F,
Time Error in fixSigDigits: @digits must be between 1 a hour
4 mil, 50% RH; ASMT D1204
 
Optical PropertiesMetricEnglishComments
Haze <= 1.0 %
@Thickness 0.102 mm
<= 1.0 %
@Thickness 0.00400 in
ASTM D1003
 
Descriptive Properties
Yield3285 in2/lb4 mil, 50% RH

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Honeywell ACLAR® CX 130E Heat Sealable PCTFE Film
Honeywell ACLAR® UltRx 2000 CTFE Homopolymer, Barrier Film
Chemours 340 PFA Perfluoroalkoxy Copolymer
Honeywell ACLAR® 11A (8.00 mil) CTFE Homopolymer, Barrier Film
Honeywell ACLAR® Cx™ 8A Heat Sealable, Co-Extruded CTFE Film

PHONWL127 / 179672

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.