MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Celanese 220 LDPE polymer for molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: 220 is a natural homopolymer, recommended for higher pressure series pipe applications such as municipal water service pipe. This LDPE resin may be safely used as articles or components of articles intended for uses in contact with food as provided in FDA regulation 21 CFR 177.1520 - Olefin polymers, and its specifications 2.2, subject to extraction limitations on the finished food-contact article as specified in that regulation. Additives:

Applications: Tubes & Pipes

Information provided by Celanese Corporation.

Key Words: higher pressure series pipe applications such as municipal water service pipe
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.921 g/cc0.0333 lb/in³AT Plastics PTM-03
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 95.595.5ASTM D2240
Hardness, Shore D 4747ASTM D2240
Tensile Strength at Break 15.0 MPa2180 psiType IV (50 mm/min); ASTM D638
Elongation at Break 550 %550 %Type IV (50 mm/min); ASTM D638
Flexural Modulus, 1% Secant 215 MPa31200 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 112 °C234 °FDSC; ASTM D3417
Vicat Softening Point 94.0 °C201 °FASTM D1525
Brittleness Temperature -82.0 °C-116 °FASTM D746
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aclo Accucomp Polyethylene LD0109L Low Density
Celanese AT 234 Low Density Polyethylene (LDPE)
Kazanorgsintez 107-22 Composition of Low Density Polyethylene, Crack-Proof
LG Chemical SEETEC BF500 LDPE
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade

PATEVB76 / 26032

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.