MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Arkema Cristamid® MS 1700 Semi-Aromatic Nylon (PASA) (Dry)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Flame Retardant; Nylon, Aromatic

Material Notes: Designation ISO 1874-PA12/xx,M,12-020

Semi-aromatic polyamide (PASA) grade for injection molding.

Transparency even thick. Outstanding thermal properties due to its high glass temperature. Good chemical resistance. Dimensional stability.

Example applications: Oil casing.

ISO data provided by the manufacturer, Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³
Water Absorption 3.2 %3.2 %
High Load Melt Index 4.9 g/10 min
@Load 21.6 kg,
Temperature 235 °C
4.9 g/10 min
@Load 47.6 lb,
Temperature 455 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 78.0 MPa11300 psi50 mm/min
Elongation at Break >= 50 %>= 50 %Nominal Strain; 50 mm/min
Elongation at Yield 8.0 %8.0 %50 mm/min
Tensile Modulus 2.11 GPa306 ksi1 mm/min
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 170 °C338 °F10°C/min
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
Oxygen Index 26 %26 %
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %Mfr. reports 'Transparent' but doesn't quantify.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Cristamid® MS 1100 Semi-Aromatic Nylon (PASA) (Dry)
Toyobo GLAMIDE® TY-502NZ 6T-Nylon
Arkema Cristamid® MS 1100 Semi-Aromatic Nylon (PASA) (Conditioned)
Arkema Cristamid® MS 1300 Semi-Aromatic Nylon (PASA) (Dry)
Toyobo GLAMIDE® TY-791HT 6T-Nylon

PZARKG229 / 25519

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.