MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 683 HEC FR Acrylonitrile Butadiene Styrene (ABS), Nickel-Coated Carbon Fiber - Flame Retardant - Electrically Conductive
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.44 g/cc1.44 g/ccASTM D 792
Additive Loading 20 %20 %Primary Additive
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 95.1 MPa13800 psiASTM D 638
Elongation at Break 1.0 %1.0 %ASTM D 638
Tensile Modulus 10.7 GPa1550 ksiASTM D 638
Flexural Strength 141 MPa20500 psiASTM D 790
Flexural Modulus 10.0 GPa1450 ksiASTM D 790
Izod Impact, Notched 0.534 J/cm
@Thickness 3.20 mm
1.00 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 3.20 J/cm
@Thickness 3.20 mm
6.00 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1.0 ohm-cm<= 1.0 ohm-cmASTM D 257
Surface Resistance <= 100 ohm<= 100 ohmESD STM11.11
Surface Resistivity per Square <= 1000 ohm<= 1000 ohmASTM D 257; ESD STM11.11
Static Decay <= 0.50 sec<= 0.50 secFTMS101C; 4046.1
Shielding Effectiveness  72 dB
@Thickness 2.00 mm,
Frequency 3.00e+7 Hz
72 dB
@Thickness 0.0787 in,
Frequency 3.00e+7 Hz
ASTM D 4935
 75 dB
@Thickness 2.00 mm,
Frequency 1.50e+8 Hz
75 dB
@Thickness 0.0787 in,
Frequency 1.50e+8 Hz
ASTM D 4935
 79 dB
@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
79 dB
@Thickness 0.0787 in,
Frequency 3.00e+8 Hz
ASTM D 4935
 82 dB
@Thickness 2.00 mm,
Frequency 5.00e+8 Hz
82 dB
@Thickness 0.0787 in,
Frequency 5.00e+8 Hz
ASTM D 4935
 85 dB
@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
85 dB
@Thickness 0.0787 in,
Frequency 7.00e+8 Hz
ASTM D 4935
 88 dB
@Thickness 2.00 mm,
Frequency 1e+9 Hz
88 dB
@Thickness 0.0787 in,
Frequency 1e+9 Hz
ASTM D 4935
 91 dB
@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
91 dB
@Thickness 0.0787 in,
Frequency 1.30e+9 Hz
ASTM D 4935
 92 dB
@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
92 dB
@Thickness 0.0787 in,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 - 238 °C400 - 460 °F
Mold Temperature 62.8 - 85.0 °C145 - 185 °F
Drying Temperature 82.2 °C
@Time 7200 sec
180 °F
@Time 2.00 hour
Moisture Content 0.10 %0.10 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PQZPA48547 / 279725

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.