MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

WI-52 Cast Cobalt Alloy
Categories: Metal; Superalloy; Cobalt Base

Material Notes: Typical applications: gas turbine parts, nozzle vanes

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  53.8 MPa
@Temperature 982 °C,
Time 3.60e+6 sec
7800 psi
@Temperature 1800 °F,
Time 1000 hour
 79.3 MPa
@Temperature 982 °C,
Time 360000 sec
11500 psi
@Temperature 1800 °F,
Time 100 hour
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.45 %0.45 %
Chromium, Cr 21 %21 %
Cobalt, Co <= 61.55 %<= 61.55 %Balance
Iron, Fe 2.0 %2.0 %
Manganese, Mn <= 0.50 %<= 0.50 %
Nickel, Ni >= 1.0 %>= 1.0 %
Niobium, Nb (Columbium, Cb) 2.0 %2.0 %
Silicon, Si <= 0.50 %<= 0.50 %
Tungsten, W 11 %11 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MetalTek MTEK 31 UNS R30031 Cobalt Base Alloy
MetalTek MAR-M-247® Centri-Vac Nickel Cobalt Based Alloy
MAR-M322 Cast Cobalt Alloy (UNS R30023)
MAR-M302 Cast Cobalt Alloy
Low Cobalt Steel Hard Magnetic Alloy

NZ97086 / 191478

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.