MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Graft Polymer GRAFTABOND™ PO-MAH 00410 IM Polyethylene Octene grafted with Maleic Anhydride
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: GRAFTABOND™ PO-MAH 00410 IM is a high performance maleic anhydride grafted ethylene copolymer. The high degree of grafting adds polarity to PE matrices, which greatly improves compatibility with fibers, fillers and PE/PA blends. It is also an excellent additive for material toughening, increasing impact strength and flexural properties.

Applications:

  • all polyamide blends
  • Standard toughening agent (golf balls, cable compounds…)
  • compatibilizing non-halogen flame retardant fillers in polymer compounds.
Supplied as: Granulate.

Properties can be regulated to customer needs.

Information provided by Graft Polymer LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 3.0 - 6.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.0 - 6.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Descriptive Properties
Drying Loss<0.5 g/cc. ASTM D6980. @ 105°C
Maleic Anhydride Graft Level0.5 to 1.3%, FTIR Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Graft Polymer GRAFTABOND™ PPC-GMA 02030 C Polypropylene grafted with Glycidyl Methacrylate
Graft Polymer GRAFTABOND™ PO-GMA 00617 Polyethylene Octene grafted with glycidyl methacrylate
Graft Polymer GRAFTABOND™ MB-EGMA 00615 Polyethylene Based Masterbatch with Glycidyl Methacrylate
Graft Polymer GRAFTABOND™ LD-MAH 02030 C Highly functionalized polyethylene with maleic anhydride
Graft Polymer GRAFTABOND™ LD-MAH 00130 TL Highly functionalized polyethylene with maleic anhydride

PGRAFT928 / 232359

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.