MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECACOMP PET TRM black 1015083 PET, Carbon Fiber Reinforced, PTFE Filled
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); PET + Carbon Fiber

Material Notes:
  • very good bearing and wear properties
Target Industries:
  • automotive industry
  • mechanical engineering

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Bulk Density 0.670 g/cc0.0242 lb/in³EN ISO 60
Density 1.50 g/cc0.0542 lb/in³
Water Absorption at Saturation <= 0.10 %<= 0.10 %50 % relative humidity up to saturation; DIN EN ISO 62
Linear Mold Shrinkage, Flow 0.0024 cm/cm0.0024 in/inDIN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.0079 cm/cm0.0079 in/inDIN EN ISO 294-4
Melt Flow 85 g/10 min
@Load 5.00 kg,
Temperature 280 °C
85 g/10 min
@Load 11.0 lb,
Temperature 536 °F
DIN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 175 MPa25400 psi50 mm/min; DIN EN ISO 527-1
Elongation at Break 2.0 %2.0 %50 mm/min; DIN EN ISO 527-1
Modulus of Elasticity 14.5 GPa2100 ksi50 mm/min; DIN EN ISO 527-1
Charpy Impact Unnotched 2.50 J/cm²11.9 ft-lb/in²DIN EN ISO 179-1eU
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 130000 ohm-cm130000 ohm-cmDIN EN ISO 3915
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  8.00 µm/m-°C
@Temperature 80.0 - 110 °C
4.44 µin/in-°F
@Temperature 176 - 230 °F
DIN EN ISO 11359-1;2
 12.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
6.67 µin/in-°F
@Temperature 73.4 - 140 °F
DIN EN ISO 11359-1;2
CTE, linear, Transverse to Flow  75.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
41.7 µin/in-°F
@Temperature 73.4 - 140 °F
DIN EN ISO 11359-1;2
 124 µm/m-°C
@Temperature 80.0 - 110 °C
68.9 µin/in-°F
@Temperature 176 - 230 °F
DIN EN ISO 11359-1;2
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°Fthrough-plane; ISO 22007-4:2008
 1.40 W/m-K9.72 BTU-in/hr-ft²-°Fin-plane; ISO 22007-4:2008
Melting Point 255 °C491 °FDIN 53765
Maximum Service Temperature, Air 110 °C230 °Flong term
 170 °C338 °Fshort term
Deflection Temperature at 0.46 MPa (66 psi) 255 °C491 °FISO-R 75 Method B
Deflection Temperature at 1.8 MPa (264 psi) 235 °C455 °FISO-R 75 Method A
Glass Transition Temp, Tg 70.0 °C158 °FDIN 53765
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 - 280 °C500 - 536 °FCylinder
Melt Temperature 270 - 280 °C518 - 536 °FMaterial temperature
Mold Temperature 130 - 160 °C266 - 320 °F
Drying Temperature <= 120 °C<= 248 °F
Dry Time 3.00 - 6.00 hour3.00 - 6.00 hour
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIO9105 / 319033

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.