MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Celanese Rynite® SST35 NC010 PET-HIGF35
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 40% Glass Reinforced

Material Notes:

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.52 g/cc0.0549 lb/in³ISO 1183
Melt Density 1.40 g/cc
@Temperature 285 °C
0.0506 lb/in³
@Temperature 545 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 90.0 MPa13100 psiISO 527-1/-2
Elongation at Break 6.0 %6.0 %ISO 527-1/-2
Tensile Modulus 7.50 GPa1090 ksiISO 527-1/-2
Compressive Strength 80.0 MPa11600 psiISO 604
Poissons Ratio 0.340.34
Shear Strength 40.0 MPa5800 psiASTM D 732
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 500 V500 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Transverse to Flow 130 µm/m-°C72.2 µin/in-°FISO 11359-1/-2
Specific Heat Capacity 1.70 J/g-°C
@Temperature 285 °C
0.406 BTU/lb-°F
@Temperature 545 °F
Melt
Thermal Conductivity 0.210 W/m-K
@Temperature 285 °C
1.46 BTU-in/hr-ft²-°F
@Temperature 545 °F
Melt
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
IEC 60695-11-10
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
<= 3.15 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 290 °C518 - 554 °FRange, Injection
 285 °C545 °FOptimum, Injection
Mold Temperature 75.0 - 95.0 °C167 - 203 °FInjection
 95.0 °C203 °FOptimum, Injection
Ejection Temperature 170 °C338 °FInjection
Drying Temperature 120 °C248 °FInjection
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.020 %<= 0.020 %Injection
Hold Pressure >= 80.0 MPa>= 11600 psiInjection
 
Descriptive Properties
AdditivesRelease agent
Back pressureAs low as possible
Drying RecommendedyesInjection
Eff. thermal diffusivity (m²/s)1.2E-07
FMVSS ClassBISO 3795 (FMVSS 302)
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>PET-HIGF35<ISO 11469
PolymerPET-I-GF35
Processing Hold Pressure Time (s/mm)4Injection
Resin IdentificationPET-HIGF35ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX4854 / 256303

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.