MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

DS-Niclel Nickel Superalloy Sheet
Categories: Metal; Superalloy; Nickel Base

Material Notes: Typical Applications: Jet engine parts.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  51.0 MPa
@Temperature 1090 °C,
Time 3.60e+6 sec
7400 psi
@Temperature 2000 °F,
Time 1000 hour
Estimated from limited data using the Larson-Miller time-temperature parameter
 61.4 MPa
@Temperature 1090 °C,
Time 360000 sec
8900 psi
@Temperature 2000 °F,
Time 100 hour
Estimated from limited data using the Larson-Miller time-temperature parameter
 70.3 MPa
@Temperature 982 °C,
Time 3.60e+6 sec
10200 psi
@Temperature 1800 °F,
Time 1000 hour
Estimated from limited data using the Larson-Miller time-temperature parameter
 84.1 MPa
@Temperature 982 °C,
Time 360000 sec
12200 psi
@Temperature 1800 °F,
Time 100 hour
Estimated from limited data using the Larson-Miller time-temperature parameter
 121 MPa
@Temperature 816 °C,
Time 3.60e+6 sec
17500 psi
@Temperature 1500 °F,
Time 1000 hour
Estimated from limited data using the Larson-Miller time-temperature parameter
 131 MPa
@Temperature 816 °C,
Time 360000 sec
19000 psi
@Temperature 1500 °F,
Time 100 hour
Estimated from limited data using the Larson-Miller time-temperature parameter
 155 MPa
@Temperature 649 °C,
Time 3.60e+6 sec
22500 psi
@Temperature 1200 °F,
Time 1000 hour
Estimated from limited data using the Larson-Miller time-temperature parameter
 162 MPa
@Temperature 649 °C,
Time 360000 sec
23500 psi
@Temperature 1200 °F,
Time 100 hour
Estimated from limited data using the Larson-Miller time-temperature parameter
 
Component Elements PropertiesMetricEnglishComments
Nickel, Ni 97.9 %97.9 %As Balance
 
Descriptive Properties
ThO2 (%)2.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kennametal Stellite Deloro® 29 Nickel Alloy
IN-162 Cast Nickel Superalloy
High-Leaded Tin Bronze, UNS C94300, Copper Casting Alloy
B. 1900 Cast Nickel Superalloy
ATI Allvac® Nickelvac® H-X Nickel Superalloy, Heat Treatment: 1177°C (2150°F) Anneal

NZ97004 / 191405

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.