System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Solvay THORNEL® P-25 Pitch-Based Fiber
Categories:
Carbon
;
Carbon Fiber/Carbon Fibre
Material Notes:
THORNEL® P25 is a continuous pitch-based carbon fiber. THORNEL P25 is offered both with and without sizing. THORNEL P25 is offered in both twisted and never-twisted forms.
Information provided by Cytec, subsequently acquired by Solvay.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.90
g/cc
0.0686
lb/in³
4K
1.92
g/cc
0.0694
lb/in³
2K
Mechanical Properties
Metric
English
Comments
Tensile Strength
1550
MPa
225000
psi
2K
1550
MPa
225000
psi
4K
Elongation at Break
0.90 %
0.90 %
2K
0.90 %
0.90 %
4K
Tensile Modulus
159
GPa
23100
ksi
2K
172
GPa
24900
ksi
4K
Thermal Properties
Metric
English
Comments
CTE, linear
-0.600
µm/m-°C
-0.333
µin/in-°F
2K
-0.600
µm/m-°C
-0.333
µin/in-°F
4K
Thermal Conductivity
26.0
W/m-K
180
BTU-in/hr-ft²-°F
4K
36.0
W/m-K
250
BTU-in/hr-ft²-°F
2K
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Solvay THORNEL® VMX-24 Pitch-Based Fiber
Solvay Thornel® Mat VMD Carbon Fiber
Solvay Thornel® Mat VMA Carbon Fiber
Solvay Thornel® P-25 2K Carbon Fiber, Pitch Precursor
Solvay THORNEL® P-55 Pitch-Based Fiber
PCYTED064 / 180366
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.