MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, PTFE-Filled

Material Notes: Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistant
Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine Tools

Information provided by Zedex

Key Words: PEEK, PTFE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³ISO 1183
Water Absorption 0.050 %
@Temperature 23.0 °C
0.050 %
@Temperature 73.4 °F
RMC 93%; DIN EN ISO 62
Moisture Absorption at Equilibrium 0.10 %0.10 %DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A >= 100>= 100DIN 53505
Hardness, Shore D 8888DIN 53505
Ball Indentation Hardness 231 MPa33500 psiDIN 2039
Tensile Strength 142 MPa20600 psiDIN EN ISO 527
Tensile Strength, Yield 64.0 MPa9280 psiElastic Limit
 120 MPa17400 psiDIN EN ISO 527
Tensile Stress at Strain 44.0 MPa
@Strain 1 %,
Time 3.60e+6 sec
6380 psi
@Strain 1 %,
Time 1000 hour
DIN 53444
Elongation at Break 4.5 %4.5 %
 4.5 %4.5 %DIN EN ISO 527
Elongation at Yield 3.9 %3.9 %Elongation at Maximum Force; DIN EN ISO 527
Tensile Modulus 7.80 GPa1130 ksiDIN EN ISO 527
Flexural Strength 150 MPa21800 psiOuter Fiber Stress at 3.5% Outer Fiber Strain; DIN EN ISO 178
 210 MPa30500 psiDIN EN ISO 178
Flexural Modulus 7.00 GPa1020 ksiDIN EN ISO 178
Compressive Yield Strength 123 MPa17800 psiElastic Limit
Compressive Strength  60.0 MPa
@Time 3.60e+7 sec
8700 psi
@Time 10000 hour
 109 MPa
@Time 360000 sec
15800 psi
@Time 100 hour
 131 MPa
@Time 36.0 sec
19000 psi
@Time 0.0100 hour
 95.0 MPa
@Strain 3.5 %
13800 psi
@Strain 3.5 %
DIN EN ISO 604
Compressive Modulus 5.454 GPa791.0 ksiDIN EN ISO 604
Fatigue Strength 105 MPa
@# of Cycles 1.00e+6
15200 psi
@# of Cycles 1.00e+6
1 Hz
K Factor (ISO)  0.40 µm/km
@Temperature 20.0 °C
0.40 µm/km
@Temperature 68.0 °F
 1.8 µm/km
@Temperature 100 °C
1.8 µm/km
@Temperature 212 °F
 3.6 µm/km
@Temperature 200 °C
3.6 µm/km
@Temperature 392 °F
 5.2 µm/km
@Temperature 240 °C
5.2 µm/km
@Temperature 464 °F
Charpy Impact Unnotched 2.30 J/cm²10.9 ft-lb/in²EN ISO 179/1eU
Charpy Impact, Notched 0.930 J/cm²4.43 ft-lb/in²EN ISO 179/1eA
Coefficient of Friction, Dynamic  0.080
@Temperature 100 °C
0.080
@Temperature 212 °F
Dry Operation
 0.10
@Temperature 20.0 °C
0.10
@Temperature 68.0 °F
Dry Operation
Coefficient of Friction, Static 0.12
@Temperature 20.0 °C
0.12
@Temperature 68.0 °F
Dry Operation
Tensile Creep Modulus, 1000 hours 4560 MPa661000 psiAt 1% Deformation; DIN 53444
Limiting Pressure Velocity 0.250 MPa-m/sec7140 psi-ft/minv = 1m/min
 0.350 MPa-m/sec9990 psi-ft/minv = 100m/min
 0.46667 MPa-m/sec13323 psi-ft/minv = 200m/min
 0.635 MPa-m/sec18100 psi-ft/minv = 10m/min
Compression Set 4.8 %4.8 %Elastic Compression Limit
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 30000 ohm-cm30000 ohm-cmIEC 93
Surface Resistance 19000 ohm19000 ohmIEC 93
Dielectric Constant 3.3
@Frequency 110 Hz
3.3
@Frequency 110 Hz
IEC 250
Dissipation Factor 0.00400.0040IEC 112
 0.061
@Frequency 110 Hz
0.061
@Frequency 110 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear  35.0 µm/m-°C
@Temperature <=100 °C
19.4 µin/in-°F
@Temperature <=212 °F
ISO E 830
 38.0 µm/m-°C
@Temperature <=150 °C
21.1 µin/in-°F
@Temperature <=302 °F
ISO E 831
Specific Heat Capacity 1.06 J/g-°C0.253 BTU/lb-°FDSC
Thermal Conductivity 0.240 W/m-K1.67 BTU-in/hr-ft²-°FDIN 52612
Melting Point 340 °C644 °FDSC
Maximum Service Temperature, Air 140 °C284 °FPressed Bushings
 250 °C482 °FContinuous
 260 °C500 °FShort Term (3h)
Deflection Temperature at 1.8 MPa (264 psi) 270 °C518 °FDIN EN ISO 75
Glass Transition Temp, Tg 146 °C295 °FDSC
Flammability, UL94 V-0V-0
Oxygen Index 43 %43 %DIN EN ISO 4589
 
Descriptive Properties
Alignment Adjustment1Nominal Scale: 1, low; 10, high
Chemical Sterilization10Nominal Scale: 1, low; 10, high
ColorAnthracite
Creep Resistance7Nominal Scale: 1, low; 10, high
Dimensional Stability with Thermal Expansion7Nominal Scale: 1, low; 10, high
Free from SiliconApplicable
Gamma-rays Radiation Sterilization7Nominal Scale: 1, low; 10, high
Injection Molded PartsApplicable
Machined PartsApplicable
Moist Heat Sterilization7Nominal Scale: 1, low; 10, high
Plastic GranulesApplicable
Resistance Against dust, Dirt, Abrasive Substances10Nominal Scale: 1, low; 10, high
Resistance Against Hot Water200
Resistance to Chemicals8Nominal Scale: 1, low; 10, high
Resistant Against DisinfectantApplicable
Rods up to Øe (de)Applicable
ROHS/WEEEApplicable
Sheets up to Maximum ThicknessApplicable
Sliding Velocity100
Suitable for Outdoor Use6Nominal Scale: 1, low; 10, high
Suitable for Use in WaterApplicable
Suitable for VacuumApplicable
Tubes (hollow rods) up to Øe (de)Applicable
UV Rays Resistance9Nominal Scale: 1, low; 10, high
UV-Sterilization10Nominal Scale: 1, low; 10, high

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced
CRP Technology AMC225xe Aluminum Alloy - SiC Composite, T4 Condition
Overview of materials for Polyimide
RSP Technology RSA-7034 T6 Aluminum Super Alloy

PZEDEX09 / 122124

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.