MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Northstar Polymers MGP-D50A High Performance Polyurethane Cast Elastomer System 50D
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Liquid

Material Notes: This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires some load-bearing, slide abrasion, constant water contact and high elongation with high energy properties. Possible applications for this material include roller skate wheels, bumpers, abrasion resistant liners and parts, rock/sand sizing screens and other specialty applications. This is a conventional “full-prepolymer” type material cured with 1,4 BDO. Can be approved for FDA dry food contact.

Information provided by Northstar Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5050ASTM D2240
Tensile Strength 28.3 MPa4100 psiASTM D412
Elongation at Break 250 %250 %ASTM D412
100% Modulus 13.8 MPa
@Strain 100 %
2000 psi
@Strain 100 %
ASTM D412
Rebound 30 %30 %Bashore Rebound; ASTM D2632
Tear Strength 39.4 kN/m225 pliSplit; ASTM D624
 107 kN/m610 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 9090ASTM D4060
 
Processing PropertiesMetricEnglishComments
Processing Temperature 25.0 °C77.0 °FCuring Agent Temperature
 82.2 - 93.3 °C180 - 200 °FPrepolymer Temperature
Mold Temperature 82.2 - 93.3 °C180 - 200 °F
Cure Time  30.0 min
@Temperature 93.3 °C
0.500 hour
@Temperature 200 °F
De-mold Time
 960 min
@Temperature 82.2 °C
16.0 hour
@Temperature 180 °F
Complete Cure Cycle
Pot Life 2.50 - 3.00 min2.50 - 3.00 min
 
Descriptive Properties
Curing AgentBNA-005
PrepolymerMGA-036
Weight Ratio1:0.119Prepolymer to Curing Agent Ratio

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alliance Polymers Zythane™ 4060A Thermoplastic Polyurethane Elastomer
Mearthane Durethane™ C 50D Polyurethane
Mearthane Durethane™ S DS-570D Solid Polyurethane Elastomer
BCC Products LIK-WOOD BC 8007 Urethane Casting
BCC Products Kwik Kast BC 8002 Urethane Casting

PNORTH03 / 54838

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.