MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Chevron Phillips Marlex® HHM TR-418Q MDPE Hexene Copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Extruded

Material Notes: High performance MDPE resin has been formulated for the demanding requirements of pressure pipe applications. Meets ASTM D4976 PE 225. Meets FDA Regulation 177.1520, suitable for food packaging applications. When blended with yellow concentrate, this resin meets ASTM D3350-99 Class 234363E; PPI Recommended Designation PE 2406; and is not recommended for food applications.

Characteristics: outstanding resistance to slow crack growth, contains UV stabilizer, outstanding pipe ring ESCR

Applications: pipe for gas distribution, oil field and other industrial pipe

Data provided by Chevron Phillips Chemical Company, LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.939 g/cc0.0339 lb/in³ASTM D1505
ESCR 100% Igepal® >= 5000 hour>= 5000 hourCond. A, B, and C; F50; ASTM D1693
 >= 5000 hour>= 5000 hourPipe Ring; ASTM F1278
Melt Flow 0.20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.20 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
High Load Melt Index 20 g/10 min
@Load 21.6 kg,
Temperature 190 °C
20 g/10 min
@Load 47.6 lb,
Temperature 374 °F
High Load; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
PENT >= 1000 hour>= 1000 hourASTM F1473
Tensile Strength at Break 33.1 MPa4800 psiType IV; 50 mm per min; ASTM D638
Tensile Strength, Yield 19.3 MPa2800 psiType IV; 50 mm per min; ASTM D638
Elongation at Break >= 500 %>= 500 %Type IV; 50 mm per min; ASTM D638
Flexural Modulus 0.621 GPa90.0 ksiASTM D3350
 0.758 GPa110 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -90.0 °C<= -130 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 193 - 216 °C379 - 421 °FStock

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Petromont 2100 Medium Density Polyethylene Resin
Borealis Borstar® FB1350 Medium Density Polyethylene
Chevron Phillips Marlex® HHM TR-305 Medium density hexene copolymer
Chevron Phillips Marlex® HHM TR-130 MDPE Film Resin
Chevron Phillips Marlex® K307 MDPE Hexene Copolymer

PCHEVM40 / 20330

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.