MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

DuPont Mobility and Materials Delrin® SC699 NC010 POM  (discontinued **)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Silicone Lubricated Low Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for the Healthcare Industry

Information provided by DuPont; The Delrin product line was sold by DuPont in 2023 but this specific grade was discontinued prior to the sale

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ISO 1183
Water Absorption 1.0 %
@Thickness 2.00 mm
1.0 %
@Thickness 0.0787 in
Sim. to ISO 62
Moisture Absorption 0.240 %
@Thickness 2.00 mm
0.240 %
@Thickness 0.0787 in
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.019 cm/cm0.019 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.018 cm/cm0.018 in/inISO 294-4, 2577
Melt Flow 25 g/10 min25 g/10 minISO 1133
 21 g/10 min
@Load 2.16 kg,
Temperature 190 °C
21 g/10 min
@Load 4.76 lb,
Temperature 374 °F
cm³/10min Volumetric Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9191ISO 2039-2
Hardness, Rockwell R 119119ISO 2039-2
Tensile Strength, Yield 63.0 MPa9140 psiISO 527-1/-2
Elongation at Break 30 %30 %ISO 527-1/-2
Elongation at Yield 15 %15 %ISO 527-1/-2
Tensile Modulus 3.10 GPa450 ksiISO 527-1/-2
Flexural Yield Strength 82.0 MPa
@Strain 3.5 %
11900 psi
@Strain 3.5 %
ISO 178
Flexural Modulus 3.00 GPa435 ksiISO 178
Poissons Ratio 0.370.37ISO 527-1/-2
Charpy Impact Unnotched  16.0 J/cm²
@Temperature 23.0 °C
76.1 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 17.5 J/cm²
@Temperature -30.0 °C
83.3 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.650 J/cm²
@Temperature 23.0 °C
3.09 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 0.750 J/cm²
@Temperature -30.0 °C
3.57 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
Coefficient of Friction, Dynamic 0.100.101h against itself; ASTM 1894
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 100 µm/m-°C55.6 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 105 µm/m-°C58.3 µin/in-°FISO 11359-1/-2
Melting Point 178 °C352 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 160 °C320 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FISO 75-1/-2
Flame Spread 28.0 mm/min
@Thickness 1.00 mm
1.10 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 220 °C410 - 428 °FInjection
 215 °C419 °FInjection Optimum
Mold Temperature 80.0 - 100 °C176 - 212 °FInjection
 90.0 °C194 °FInjection Optimum
Drying Temperature 80.0 °C176 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourDehumidified Dryer; Injection
Moisture Content 0.050 %0.050 %Injection
Hold Pressure 80.0 - 100 MPa11600 - 14500 psiInjection
Annealing Temperature 160 °C320 °FInjection
 
Descriptive Properties
AdditivesLubricants
 Release agent
Annealing time30 min/mmInjection - Optional
Delivery formPellets
Drying RecommendedyesInjection
Hold pressure time (s/mm)8Injection
Part Marking CodePOMISO 11469
ProcessingInjection Molding
Resin IdentificationPOMISO 1043

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® 2205 Polycarbonate, Injection Grade
Delrin Delrin® SC655 NC010 POM
INEOS Styrolution Novodur® P2H-AT Acrylonitrile Butadiene Styrene (ABS)
Celanese Hostaform® MT12U03 POM, Medical Technology
Delrin Delrin® 500AL NC010 POM-S

PDSX5165 / 197805

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.