MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Titanium Ti-5Al-2Sn-2Zr-4Mo-4Cr (Ti-17) Alpha-Beta Processed
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: Information provided by Allvac and the references. Beta Transus 890ºC ; Alpha-Beta Alloy; Double Solution Treated 860ºC, 2h; 800ºC, 4h; Aged 620ºC, 8h.

Applications: Compressor discs, heavy section forgings for gas turbine engine components.

Characteristics: High tensile strength, good crack growth/fatigue resistance and good fracture toughness.

Forms typically available: Billet and bar.

1 other heat treatment of this alloy is in MatWeb.

Key Words: UNS R58650
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 4.65 g/cc0.168 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 369369Estimated from Rockwell C.
Hardness, Knoop 403403Estimated from Rockwell C.
Hardness, Rockwell C 4040
Hardness, Vickers 386386Estimated from Rockwell C.
Tensile Strength 1000 MPa
@Temperature 316 °C
145000 psi
@Temperature 601 °F
Tensile Strength, Ultimate 1185 MPa171900 psi
Tensile Strength, Yield 1140 MPa165000 psi
Elongation at Break 8.0 %8.0 %
Creep Strength 724 MPa
@Temperature 316 °C,
Time >=3.60e+6 sec
105000 psi
@Temperature 601 °F,
Time >=1000 hour
strain 0.2%
Rupture Strength 910 MPa
@Temperature 316 °C,
Time 3.60e+6 sec
132000 psi
@Temperature 601 °F,
Time 1000 hour
Modulus of Elasticity 115 GPa16700 ksi
Notched Tensile Strength 1480 MPa215000 psiKt (stress concentration factor) = 4.0
Poissons Ratio 0.330.33Typical for alpha-beta titanium alloy.
Fatigue Strength  725 MPa
@# of Cycles 100000
105000 psi
@# of Cycles 100000
disk forging
 745 MPa
@# of Cycles 5000
108000 psi
@# of Cycles 5000
disk forging
Fracture Toughness 35.0 MPa-m½31.9 ksi-in½K(IC)
Shear Modulus 43.2 GPa6270 ksiCalculated from typical values.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000160 ohm-cm0.000160 ohm-cmEstimated from similar alpha-beta titanium alloys.
 
Thermal PropertiesMetricEnglishComments
CTE, linear  8.50 µm/m-°C
@Temperature 20.0 - 100 °C
4.72 µin/in-°F
@Temperature 68.0 - 212 °F
Typical alpha-beta titanium alloy
 9.70 µm/m-°C
@Temperature 20.0 - 400 °C
5.39 µin/in-°F
@Temperature 68.0 - 752 °F
average
Specific Heat Capacity 0.525 J/g-°C0.125 BTU/lb-°FTypical value for titanium alloys.
Thermal Conductivity 7.80 W/m-K54.1 BTU-in/hr-ft²-°F
Beta Transus 890 °C1630 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 5.0 %5.0 %
Chromium, Cr 4.0 %4.0 %
Hydrogen, H <= 0.0125 %<= 0.0125 %
Iron, Fe <= 0.30 %<= 0.30 %
Molybdenum, Mo 4.0 %4.0 %
Nitrogen, N <= 0.040 %<= 0.040 %
Oxygen, O 0.080 - 0.13 %0.080 - 0.13 %
Tin, Sn 2.0 %2.0 %
Titanium, Ti 83 %83 %
Zirconium, Zr 2.0 %2.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Ti-5Al-2Sn-2Zr-4Mo-4Cr (Ti-17) Beta Processed
ATI Allvac® Ti-17 Titanium Alloy, Heat Treatment: 899°C (1650°F) + Age
Titanium Ti-6Al-2Sn-2Zr-2Mo-2Cr-.25Si Alpha-Beta Processed + Aged
ATI Allegheny Ludlum Grade 23 (6-4 ELI) Titanium (UNS R56401)
Titanium Ti-6Al-2Sn-4Zr-6Mo (Ti-6-2-4-6) STA-1

MTP171 / 14227

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.