16 mm ACRYLITER Alltop high impact acrylic double-skin sheet is a light transmitting, heat-insulating and weatherresistant double-skin sheet made of impact-modified acrylic (polymethyl methacrylate, PMMA) polymer. It was designed as an interior or exterior glazing panel for commercial, institutional, educational and research Greenhouses where high light levels, greater optics and impact resistance are desired. Also ideal for interior or exterior commercial and architectural construction. Advantages of 16 mm ACRYLITE® Alltop high impact acrylic double-skin sheet - Extraordinary clear sheet is UV-resistant and includes a 30-year warranty against yellowing.
- ACRYLITE® Alltop has a light transmission of 89%.
- ACRYLITE® Alltop‘s patented no drip coating is applied on every surface, including inside the flutes. The coating allows for maximum light transmission virtually eliminating all condensation droplets both inside the greenhouse and flutes.
- Hail-resistant with a 10-year warranty for withstanding hailstones with a kinetic energy of 1 joule.
- Up to 50% better energy savings over single layer glazings.
Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH. |