MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECASINT 6032 black Polyimide, Graphite Filled
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Graphite Filled

Material Notes:
  • very good thermal stability
  • very good bearing and wear properties
  • good wear resistance
  • low thermal expansion
  • high creep resistance
  • high dimensional stability
  • sensitive to hydrolysis in higher thermal range
Target Industries:
  • hot glass technology
  • mechanical engineering
  • aircraft and aerospace technology
  • automotive industry

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.57 g/cc0.0567 lb/in³
Water Absorption 0.30 %
@Time 86400 sec
0.30 %
@Time 24.0 hour
DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8383DIN EN ISO 868
Tensile Strength 51.0 MPa7400 psi50 mm/min; DIN EN ISO 527-1
Elongation at Break 1.3 %1.3 %50 mm/min; DIN EN ISO 527-1
Modulus of Elasticity 5.20 GPa754 ksi1 mm/min; DIN EN ISO 527-1
Flexural Strength 70.0 MPa10200 psi10 mm/min; DIN EN ISO 178
Flexural Modulus 5.50 GPa798 ksi2 mm/min; DIN EN ISO 178
Flexural Strain at Break 1.3 %1.3 %10 mm/min; DIN EN ISO 178
Compressive Strain at Break 12 %12 %10 mm/min; EN ISO 604
Compressive Yield Strength 120 MPa
@Strain 10 %
17400 psi
@Strain 10 %
10 mm/min; EN ISO 604
Compressive Strength 125 MPa18100 psi10 mm/min; EN ISO 604
 
Thermal PropertiesMetricEnglishComments
CTE, linear  15.0 µm/m-°C
@Temperature 50.0 - 200 °C
8.33 µin/in-°F
@Temperature 122 - 392 °F
XY; DIN EN ISO 11359-1;2
 27.0 µm/m-°C
@Temperature 200 - 300 °C
15.0 µin/in-°F
@Temperature 392 - 572 °F
XY; DIN EN ISO 11359-1;2
Specific Heat Capacity 0.970 J/g-°C0.232 BTU/lb-°FDIN EN 821
Thermal Conductivity 1.66 W/m-K
@Temperature 40.0 °C
11.5 BTU-in/hr-ft²-°F
@Temperature 104 °F
DIN EN 821
Glass Transition Temp, Tg 288 °C550 °F
Flammability, UL94 V-0V-0DIN IEC 60695-11-10
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8208 / 319136

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.