MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Lucas-Milhaupt Easy-Flo 30 Brazing Alloy  (Unverified Data**)
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Formerly Silvaloy® 30. Silvaloy 30 is historically a modification of Silvaloy 35 with further reduction in silver content resulting in a higher melting point and a longer range. Silvaloy 30 is used for brazing steel, stainless steel, copper, copper alloys, nickel, nickel alloys or combinations of these metals. It is similar to Silvaloy 35 in performance although it contains less silver. Its broader melting range is helpful where clearances are not uniform. Typical applications are the joining of ferrous, nonferrous and dissimilar metals and alloys with close joint clearances.

Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).

Key Words: AWS BAg-2a
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 8.76 g/cc8.76 g/cc
Density 8.75 g/cc0.316 lb/in³
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000550 ohm-cm0.00000550 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Melting Point 607.2 - 710 °C1125 - 1310 °F
Solidus 607.2 °C1125 °F
Liquidus 710 °C1310 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 710 - 843 °C1310 - 1550 °FBrazing Temperature
 
Component Elements PropertiesMetricEnglishComments
Cadmium, Cd 19 - 21 %19 - 21 %
Copper, Cu 26 - 28 %26 - 28 %
Other, total <= 0.15 %<= 0.15 %
Silver, Ag 29 - 31 %29 - 31 %
Zinc, Zn 21 - 25 %21 - 25 %
 
Descriptive Properties
ColorLight Yellow
Electrical Conductivity (% IACS)31

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Universal Wire Works BAg-23 (AMS 4766) Silver Brazing Filler Metal
Lucas-Milhaupt Silvaloy® 255 Brazing Alloy
Lucas-Milhaupt Easy-Flo 25 Brazing Alloy
Antimony (III) Fluoride, SbF3
Lucas-Milhaupt Silvacore® A50N Flux Cored Brazing Alloy

NBRW022 / 79798

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.