MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger Tecamid® MDS® Molybdenum Disulfide Filled Nylon (PA)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Tecamid MDS® has enhanced surface lubricity and wear resistance over unfilled nylon. It is an ideal material to replace metals in machinery.
  • Low surface friction
  • Increased surface hardness
  • Increased heat resistance
  • Higher tensile properties
  • Improved dimensional stability

Information Provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ASTM D792
Water Absorption 1.2 - 2.5 %1.2 - 2.5 %at 24 hours; ASTM D570
Water Absorption at Saturation 7.5 - 8.5 %7.5 - 8.5 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Yield 75.8 MPa11000 psiASTM D638
Elongation at Break 15 %15 %ASTM D638
Tensile Modulus 3.10 GPa450 ksiASTM D638
Izod Impact, Notched 1.12 J/cm2.10 ft-lb/inASTM D256
K (wear) Factor 383 x 10-8 mm³/N-M190 x 10-10 in³-min/ft-lb-hr40 psi, 50 fpm; ASTM D3702
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Constant 2.5
@Frequency 60 Hz
2.5
@Frequency 60 Hz
ASTM D150
Dielectric Strength 1.18 kV/mm30.0 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 72.0 µm/m-°C
@Temperature 20.0 °C
40.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.67 J/g-°C0.400 BTU/lb-°F
Melting Point 255 °C491 °FASTM D2133
Maximum Service Temperature, Air 110 °C230 °FLong Term; ASTM UL746B
 179 °C355 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 243 °C470 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °FASTM D648
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, 30% Glass Fiber Filled
AISI 12L14 Steel, cold drawn, 19-38 mm round
Kinetics MIM 17-4PH Stainless Steel (As Sintered)
Kinetics MIM 17-4PH Stainless Steel (H1100 Condition)
Latitude Manufacturing PowderFlo® 17-4PH Stainless Steel Metal Injection Molding Compound

PENS84 / 35999

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.